Teledyne DALSA Launches Portable Digital Radiography System at ASNT Annual Conference

Teledyne DALSA3, Waterloo, Canada

Light-weight and ruggedized portable system enables high-resolution X-ray inspection on the go.

Long Beach, CA – October 18, 2016 - Teledyne DALSA together with Teledyne ICM, both Teledyne Technologies companies and global leaders in digital X-ray imaging technology, will showcase their Go-Scan™ Portable Digital Radiography Systems at the ASNT Annual Conference being held October 24-27th in Long Beach, California, in booth #628.

Teledyne ICM and Teledyne DALSA unite forces to reveal their first Integrated Portable Digital X-Ray Systems for Non-Destructive Testing (NDT) applications. The Go-Scan systems feature a high-definition tablet display with user-friendly touch-software for real-time imaging. Light-weight and ruggedized, the detector units and X-ray generators are housed in a shock-absorbing mechanical design, making them suitable for industrial X-ray inspection and non-destructive testing applications in the Oil & Gas, Petrochemical, Shipbuilding, Aerospace, Defense and other related industries.

The Go-Scan 1510 HR and 1510 XR portable x-ray detectors feature an active area of 102 x 153 mm (roughly 4 x 6 inches), 99 or 49.5 micron pixel size respectively, and real-time frame rates of up to 30 fps with a choice of wired Gigabit Ethernet or wireless Wi-Fi connection. The built-in rechargeable lithium-ion battery delivers up to 7 hours of continuous operation.

 
Feedback: ()

Share:
More from "Teledyne DALSA" (2)
2019-03Teledyne releases its proven high-resolution industrial x-ray detector at NDTMA’s Annual Conference
2014-06New Rad-icon Family of Large Format, High Speed CMOS X-Ray Detectors for Non Destructive Testing
... All 2 Details >
Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window