where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -
Issue '2007-12'
Vol.12 No.12 - The e-Journal of Nondestructive Testing - ISSN 1435-4934
Summary

In this month’s issue we publish the CD-Proceedings of the Annual NDT Conference of the German Society for Nondestructive

...
Testing (DGZfP) held in Fürth in May 2007. DGZfP was our partner in Internet Publishing of NDT Conference Proceedings from the earliest developments of NDT.net. We are happy to see that more and more NDT Societies recognize the benefits to the NDT community (their members!) from this concept. But this is not the case in all societies.

We visited and have been an exhibitor at the ASNT Fall Conference & Quality Testing Show in Las Vegas (News). Several authors voiced their opinion to us that they would prefer to see their papers in NDT.net. In spite of our efforts to develop a cooperation with ASNT to publish NDT technical materials, ASNT has opted to hold the materials to themselves. Hopefully a more open cooperation can be developed in future to the benefit of the entire NDT community.

Do not miss the 8 papers of individual authors we publish in this issue among the 150 DGZfP papers. Also do not miss the News Section, e.g. "Progresses in the preparation for the 17th WCNDT". Abstracts are requested until Dec. 31 2007.

New Events & Web Resources |more|
14 News in this issue
Progresses in the preparation for the 17th WCNDT
Chinese Society for Nondestructive Testing (ChSNDT)
GE Announces Weldstar Girth Weld Pipeline Inspection System
Waygate Technologies (former GE Inspection Technologies)
Physical Acoustics Corp. Provides Energy Labs with Systems to Improve Wind Turbine Performance
MISTRAS Products & Systems
New Scanner will Boost Resolution of Long-Range Pipe Inspection
Phoenix Inspection Systems Ltd
Phoenix founder Jim Quirk dies at 71
Phoenix Inspection Systems Ltd
GE?s Phasor XS Qualified by EPRI
Waygate Technologies (former GE Inspection Technologies)
Nondestructive Inspection Team Strives to Increase Reliability
Tinker Air Force Base ( AFRL/RXSST)
Tritex NDT Attend ASNT Fall Conference in Las Vegas
Tritex NDT Ltd
Carestream Health Asserts Nondestructive Testing Focus at ASNT Fall Conference
Carestream Health, Inc.
PE-900 Photo-Elastic Visualisation System - SEE SOUND
Materials Research Institute
NDT.net at ASNT Fall Conference Nov'07 in Las Vegas
NDT.net
First International Symposium on Laser-Ultrasonic
National Research Council of Canada (NRC)
ASNT's 2007 Fall Conference and Quality Testing Show
ASNT
ZfP Zeitung Dezember 2007 Ausgabe 107
Deutsche Gesellschaft für Zerstörungsfreie Prüfung (DGZfP)
Table of Contents
157 Articles in
Issue: 2007-12
Title / Author(s) / Keywords Publication
Automated Radioscopic Inspection of Aluminum Die Castings
D. Mery14
Departamento de Ciencia de la Computación; Pontificia Universidad Católica de Chile6, Santiago de Chile, Chile
Radiographic Testing (RT), Automated Defect Recognition ADR, Automated System, Aluminium, casting
NDT.net Journal
Choosing the Proper Nondestructive Testing Techniques
D. Bugden
Magnetic Analysis Corp (MAC)27, Elmsford, NY, USA
NDT-wide
NDT.net Journal
The Detection of Oblique Defects in Tubes Using Rotary Ultrasound Testers
J. Venczel2
Magnetic Analysis Corp (MAC)27, Elmsford, NY, USA
Ultrasonic Testing (UT), tubing piping
NDT.net Journal
Testing Critical Medical Tubing Using High Frequency Eddy Current Coils
T. Libby
Magnetic Analysis Corp (MAC)27, Elmsford, NY, USA
Electromagnetic Testing (ET), eddy current testing (ECT), tubing piping
NDT.net Journal
A Contribution to Phased Array Ultrasonic Inspection of Welds Part 3: Sizing Capability
P. Ciorau51
Ontario Power Generation Inc.(OPG)56, Pickering, Canada
Ultrasonic Testing (UT), phased array, weld, crack depth
NDT.net Journal
IR Thermography for the Detection of Buried Objects: A Short Review
C. Santulli20
Electrical Engineering Department; Università di Roma - La Sapienza31, Rome, Italy
Infraread Testing (IRT), thermal NDT, remote inspection
NDT.net Journal
Experimental Measurements Carried out for the Transport of Humidity in Building Material
J. Skramlik6, M. Novotny6
Faculty of Civil Engineering; Brno University of Technology (BUT)227, Brno, Czech Republic
Electromagnetic Testing (ET), civil engineering
NDT.net Journal
A Photoacoustic Study on Trichloroethylene in Water
G. Bama1, K. Ramachandran25
1Sri Meenakshi Government Arts College for Women, Madurai, India
2School of Physics; Madurai Kamaraj University6, Madurai, India
NDT-wide, Ultrasonic Testing (UT), liquid, water, materials characterization
NDT.net Journal
DGZfP 2007 Abschlussvortrag
Die Geschichte mit der Geschichte - Die Historische Kommission in der DGZfP
H. Heidt110, V. Deutsch26
1BAM Federal Institute for Materials Research and Testing1326, Berlin, Germany
2Karl Deutsch Pruef- und Messgeraetebau123, Wuppertal, Germany
Germany, DGZfP, history
DE
DGZfP 2007
Session: Abschlussvortrag
DGZfP 2007 Ausbildung
In unsere Zukunft investieren - Stand der Werkstoffprüfer-Ausbildung
H. Wessel-Segebade22
Deutsche Gesellschaft für Zerstörungsfreie Prüfung (DGZfP)163, Berlin, Germany
NDT-wide, Qualification & Certification, training, education, materials tester
DE
DGZfP 2007
Session: Ausbildung
DGZfP 2007 Automotive
Visualisierung von Randschichtfehlern in Aluminiumguss
G. Mook60, J. Simonin23, F. Michel18, M. Luther, C. Borchert
Institut für Werkstofftechnik und -prüfung; University of Magdeburg (OVGU)87, Magdeburg, Germany
Electromagnetic Testing (ET), eddy current testing probe array, Ultrasonic Testing (UT), rayleigh wave, ultrasonic imaging, lamb wave, imaging, aerospace, automotive, Aluminium, casting, plate, defect detection, hidden defects
DE
DGZfP 2007
Session: Automotive
DGZfP 2007 Automotive
Ermittlung mechanisch-technologischer Eigenschaften warmumgeformter Automobilstrukturen durch die magnet-induktive Oberwellenanalyse
H. Chojecki1, J. Nehring17, H. Engels2, C. Müller-Bollenhagen3
1Division CT; Institut Dr. Foerster2, Dortmund, Germany
2ISE Innomotive Systems Europe, Bergneustadt, Germany
3University of Siegen29, Siegen, Germany
Electromagnetic Testing (ET), Magnetic Hysteresis Loop, higher harmonics
DE
DGZfP 2007
Session: Automotive
DGZfP 2007 Automotive
Zerstörungsfreie Bestimmung der Oberflächenhärtetiefe mittels Ultraschallverfahren - Erfahrungen und notwendige Weiterentwicklungen
E. Schneider119, M. Stroh12, Y. Lejeune2
1Fraunhofer-Institute for Non-Destructive Testing (IZFP)476, Saarbrücken, Germany
2Q NET Engineering GmbH14, Saarbrücken, Germany
Ultrasonic Testing (UT), hardness testing
DE
DGZfP 2007
Session: Automotive
DGZfP 2007 Automotive
Die Rolle der zerstörungsfreien Prüfung im Produktentstehungsprozess ? Betrachtungen zu einer qualitätsgesteuerten Produktion mit sicheren Produktions- und Prüfprozessen im Automobilbau unter Einbeziehung von innovativer ZfP
K. Hanschmann5
LVQ-WP Werkstoffprüfung7, Mülheim, Germany
DE
DGZfP 2007
Session: Automotive
DGZfP 2007 Automotive
Leichtbauweise im Automobilbau forciert neue ZfP-Anwendungen
P. Buschke110, J. Wagner14, E. Leitzke22
1Waygate Technologies (former GE Inspection Technologies)313, Hürth, Germany
2Everest VIT, Ovendorf, Germany
DE
DGZfP 2007
Session: Automotive
DGZfP 2007 Automotive
Elektromagnetischer Bewegtfeldsensor zur Bildgewinnung
G. Mook60, J. Simonin23, F. Michel18
Institut für Werkstofftechnik und -prüfung; University of Magdeburg (OVGU)87, Magdeburg, Germany
Electromagnetic Testing (ET), eddy current testing probe array, eddy current testing probe, imaging, aerospace, automotive, railway, Aluminium, casting, plate, hidden corrosion, hidden defects
DE
DGZfP 2007
Session: Automotive
DGZfP 2007 Automotive
Autoflux?: Prüfautomat für Rissprüfung
E. Guttengeber8, R. Söhnchen13
Automation W+R15, Munich, Germany
Magnetic Testing (MT), Magnetic Particle Testing (MPI), Automated System, in-process
DE
DGZfP 2007
Session: Automotive
DGZfP 2007 Automotive
PROline - Ultraschallprüfung von Elektronen- bzw. Laserstrahl- geschweißten Schaltzahnrädern - und viele weitere Anwendungsbereiche in der Produktion
G. Vogt47, C. Köhler30
VOGT Ultrasonics GmbH80, Burgwedel, Germany
Ultrasonic Testing (UT), dry-coupling, automated ultrasonic testing, A-Scan, mechanized, Automated System, automotive, weld, in-process
DE
DGZfP 2007
Session: Automotive
DGZfP 2007 Automotive
BLICK INS INNERE
N. Fox1, J. Zandhuis1, G. Vogt247
13DX-Ray Ltd., Leicestershire, United Kingdom
2VOGT Ultrasonics GmbH80, Burgwedel, Germany
DE
DGZfP 2007
Session: Automotive
DGZfP 2007 Automotive
Highlights der Wirbelstromprüfung an Automobilkomponenten. Über die Vermeidung und Begrenzung von Schadensfällen
M. Junger10
Rohmann GmbH17, Frankenthal, Germany
Electromagnetic Testing (ET), eddy current testing (ECT), automotive
DE
DGZfP 2007
Session: Automotive
 
Page:
 -1-   2   3   4   5   6   7   8 
next pageNext
Actual Cooperations
Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window