11 News in this issue
BRACELET is ideal solution for small-bore pipe inspection
Phoenix Inspection Systems Ltd
Mecnov NDT Systems Acquires The Assets of Contour Dynamics, Inc.
Contour Dynamics Inspection Systems
Major Order for Fan Blade Scanner
Midas NDT Systems Ltd.
HBM makes fuselage assembly safer for modern commercial aircraft
Hottinger Baldwin Messtechnik (HBM)
AGR Field Operations launches PAUT system
Technology Design Ltd
AcousticEye Dolphin G3 Enables Advanced Tube Inspection for Heat Exchangers
AcousticEye B.V.
Olympus Introduces the In-line ERW Tube Inspection System
Olympus Scientific Solutions Americas (OSSA)
New Pipe Weld Inspection Solution from GE Increases Productivity and Reduces Inspection Constraints
GE Inspection Technologies GmbH
ASTM International Nondestructive Testing Committee Presents Charles W. Briggs Award to Dr. Clifford Bueno
ASTM International
'Smart' solutions for human skin, bridge testing and more are in largest-ever SPIE Smart Structures/NDE program
International Society for Optics and Photonics (SPIE)
ZfP Zeitung Februar 2011 Ausgabe 123
Deutsche Gesellschaft für Zerstörungsfreie Prüfung (DGZfP)
Table of Contents
89 Articles in
Issue: 2011-03
Title / Author(s) / Keywords Publication
A Contribution to Length Sizing of Saturated Amplitude for Conventional and Phased Array Ultrasonic Techniques
P. Ciorau51, J. Lam6
Inspection and Maintenance Services; Ontario Power Generation Inc.(OPG)56, Pickering, Canada

NDT.net Journal
Currents and Trends on Fiber Sensing Technologies for Structural Health Monitoring
J. Lopez-Higuera8, L. Rodríguez, A. Quintela, A. Cobo3
Photonics Engineering Group; University of Cantabria10, Santander, Spain
Ultrasonic Testing (UT), Acoustic Emission (AE), localisation of damage, Fiber optics sensors, Fiber optics sensors, aerospace, chemical and petrochemical, civil engineering, fibre reinforced materials, materials characterization, strain, Deformation, strength, structural health monitoring (SHM)

NDT.net Journal
AeroNDT 2010 Advanced Aero Structures Assessment
Advances in Industrial Testing Machines for the Automated Inspection of Aerospace Components
P. Marty7, S. Gripp15, D. Ungerer4
AREVA NDE Solutions; intelligeNDT Systems & Services GmbH & Co. KG94, Erlangen, Germany
AeroNDT 2010
Session: Advanced Aero Structures Assessment
AeroNDT 2010 Advanced Aero Structures Assessment
The Airbus SHM Development Process
C. Bockenheimer12
Testing Technology; Airbus Operations GmbH66, Bremen, Germany

AeroNDT 2010
Session: Advanced Aero Structures Assessment
AeroNDT 2010 Advanced Aero Structures Assessment
Sensors Integration during Composite Curing
R. BERTRAND1, M. Bach29, C. Boller182
1Saarland University80, Saarbrücken, Germany
2EADS Innovation Works5, Bremen, Germany
Visual and Optical Testing (VT/OT), optical fibre, aerospace, composite, fibre reinforced materials, delamination, strain, condition monitoring, flaw detection, Deformation, structural health monitoring (SHM)

AeroNDT 2010
Session: Advanced Aero Structures Assessment
AeroNDT 2010 Advanced Aero Structures Assessment
Processing of Acousto-Ultrasonic Data for Analysis of Structural Parameters in CFRP Structures
M. MOIX-BONET15, M. Bach29, C. Boller182, B. Eckstein28
1Saarland University80, Saarbrücken, Germany
2EADS Innovation Works5, Bremen, Germany
Ultrasonic Testing (UT), guided waves (lamb waves), Guided waves, aerospace, composite, carbon fiber reinforced plastic (CFRP), delamination, condition monitoring, flaw detection, structural health monitoring (SHM)

AeroNDT 2010
Session: Advanced Aero Structures Assessment
AeroNDT 2010 Automated Inspection
Comparison of Probing Error in Dimensional Measurement by Means of 3D Computed Tomography with Circular and Helical Sampling
J. Hiller121, S. Kasperl138, T. Schön118, S. Schröpfer110, D. Weiß212
1aEntwicklungszentrum Röntgentechnik bDevelopment Center X-ray technology (EZRT); Fraunhofer Institute for Integrated Circuits (IIS)185, Fürth, Germany
2Carl Zeiss Industrielle Messtechnik GmbH22, Oberkochen, Germany
Radiographic Testing (RT), 3D Computed Tomography, image quality, reconstruction algorithm, Simulation, metrology, quality control

AeroNDT 2010
Session: Automated Inspection
AeroNDT 2010 Automated Inspection
Defect Characterization and Determination of Material Properties in CFRP Specimens Using Pulsed Thermography Combined with 3D Finite Element Simulation, Computed Tomography and Ultrasonic Testing
G. Hendorfer19, G. Mayr20
Upper Austrian University of Applied Sciences (FH OÖ)171, Wels, Austria

AeroNDT 2010
Session: Automated Inspection
AeroNDT 2010 Automated Inspection
Extended Thermoelastic Stress Analysis Applied to Carbon Steel and CFRP
R. Plum14, J. Medgenberg23, M. Merzbacher3, T. Ummenhofer15
1Versuchsanstalt fuer Stahl; Karlsruhe Institute of Technology (KIT) 5, Karlsruhe, Germany
2Institut für Bauwerkserhaltung und Tragwerk; Bilfinger Berger AG, Mannheim, Germany
3Merzbacher UB, Braunschweig, Germany
Infrared Testing (IRT), lock-in thermography, carbon fiber reinforced plastic (CFRP), Carbon steel, fatigue damage

AeroNDT 2010
Session: Automated Inspection
AeroNDT 2010 Damage Tolerance & Ageing Aircraft
An Australian Perspective on the Application of Infrared Thermography to the Inspection
N. Rajic4, D. Rowlands, K. Tsoi2
Defence Science And Technology Organisation (DSTO)14, Melbourne, Victoria, Australia

AeroNDT 2010
Session: Damage Tolerance & Ageing Aircraft
AeroNDT 2010 Damage Tolerance & Ageing Aircraft
Systematic investigation on the detection limit of impact damage with thermography
H. SCHMUTZLER, A. GarcÍa, J. Meyer, H. Wittich, K. Schulte6
aInstitut für Kunststoffe und Verbundwerkstoffe bInstitut für Nachrichtentechnik; Technische Universität Hamburg-Harburg (TUHH)15, Hamburg, Germany
Infrared Testing (IRT), pulsed phase thermography, ultrasound thermography, detection, composite, carbon fiber reinforced plastic (CFRP), delamination, impact damage

AeroNDT 2010
Session: Damage Tolerance & Ageing Aircraft
AeroNDT 2010 Damage Tolerance & Ageing Aircraft
Structural Damage Detection Using Laser Vibrometers
R. Jenal1, W. Staszewski117, A. Klepka24, T. Uhl228
1Department of Mechanical Engineering; Sheffield University33, Sheffield, United Kingdom
2Department of Robotics and Mechatronics; AGH- University of Science and Technology67, Krakow, Poland
Ultrasonic Testing (UT), laser ultrasound, non-contact ultrasound, velocity, strain, vibration analysis, automated ultrasonic testing (AUT), fatigue cracks, non linear acoustics, guided waves (lamb waves), Guided waves, laser vibrometry
AeroNDT 2010
Session: Damage Tolerance & Ageing Aircraft
AeroNDT 2010 Damage Tolerance & Ageing Aircraft
Non-destructive Characterization of Composites: From Small Scale to Complex Component Testing - A Challenge
B. Müller45, V. Trappe17, J. Goebbels53, S. Hickmann7, F. Grasse
BAM Federal Institute for Materials Research and Testing1324, Berlin, Germany
x-ray diffraction, aerospace, composite, polymers, carbon fiber reinforced plastic (CFRP), crack, Fatigue Crack, imaging, Scattering, visualization, x-ray imaging, X-ray Refraction, wide angle x-ray scattering
AeroNDT 2010
Session: Damage Tolerance & Ageing Aircraft
AeroNDT 2010 Damage Tolerance & Ageing Aircraft
Application of Combined NDT Methods to Study the Helicopter Rotor Blades
M. Balasko5, G. Endröczi2, L. Horváth
aAtomic Energy Research Institute bNucleus and Particles Research Institute; MTA KFKI Budapest5, Budapest, Hungary

AeroNDT 2010
Session: Damage Tolerance & Ageing Aircraft
AeroNDT 2010 Damage Tolerance & Ageing Aircraft
Enhanced TDR Technique for Fault Detection in Electrical Wires and Cables
G. Shirkoohi, K. Hasan
Department of Engineering & Design; London South Bank University6, London, United Kingdom

AeroNDT 2010
Session: Damage Tolerance & Ageing Aircraft
AeroNDT 2010 Emerging Technologies
Terahertz Imaging for Non-Destructive Testing
J. Jonuscheit9, R. Beigang3, F. Ellrich2, J. Klier3, C. Matheis3, D. Molter, M. Theuer
Fraunhofer Institute for Physical Measurement Techniques IPM10, Kaiserslautern, Germany
Electromagnetic Testing (ET), Terahertz, aerospace, automotive, security, adhesive joint, ceramic, coating, plastic, polymers, tubes and pipes, delamination, thickness, adhesives, Fatigue, crack detection, materials analysis

AeroNDT 2010
Session: Emerging Technologies
AeroNDT 2010 Emerging Technologies
Damage Detection in Bolted Joints by Fibre Optics Distributed Sensing
A. Güemes23, A. Fernandez-Lopez11
Dpt Aeronautics.; Technical University of Madrid (UPM) 54, Madrid, Spain
Visual and Optical Testing (VT/OT), fibre optics, aerospace, joint, structural health monitoring (SHM), mechanical testing

AeroNDT 2010
Session: Emerging Technologies
AeroNDT 2010 Emerging Technologies
High Resolution Inspection of Carbon Fiber Materials by Eddy Current Techniques
H. Heuer40, M. Schulze18, N. Meyendorf36
aBranch Lab Dresden bCenter for Materials Diagnostics; Fraunhofer Institute for Ceramic Technology and System (IKTS)230, Dresden, Germany

AeroNDT 2010
Session: Emerging Technologies
AeroNDT 2010 Emerging Technologies
Development of Electromagnetic Procedures for Evaluation of CFRP Using Metamaterials
R. Grimberg150, A. Savin165, R. Steigmann155, I. Curtu24
1Nondestructive Testing Department; National Institute of R&D for Technical Physics75, Iasi, Romania
2Transilvania University13, Brasov, Romania
AeroNDT 2010
Session: Emerging Technologies
AeroNDT 2010 Emerging Technologies
Active Thermography for Quantitative NDT of CFRP Components
C. Spiessberger20, A. Dillenz20, T. Zweschper14
Edevis GmbH29, Stuttgart , Germany
Infrared Testing (IRT), lock-in thermography, Depth of Penetration, thermal NDT, frequency analysis, calibration, Automated Defect Recognition ADR, Automated System, aerospace, automotive, composite, fibre reinforced materials, thickness, quality assurance, Quantitative NDT, Quantitative, data fusion, DGZfP, Probability of Detection (POD)

AeroNDT 2010
Session: Emerging Technologies
 
Page:
 -1-   2   3   4   5 
next pageNext
Actual Cooperations
Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window