where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

Archive Authors Keywords


Publication Index



Select filters or/and search


Sort Pages
Check Filters!
New/Updated
NDT.net Journal
NDT Review
DGZfP 2019
DGZfP AE-2019
NDE-India 2018
MMM-NDT 2019
QIRT 2018
ICWNDT 2018
more >
New/UpdatedNDT.net JournalNDT ReviewDGZfP 2019DGZfP AE-2019NDE-India 2018MMM-NDT 2019QIRT 2018ICWNDT 2018 more >

NDT.net Journal |Website|

e-Journal of Nondestructive Testing (NDT) ISSN 1435-4934

Share ...     

Keywords Authors & Institutions
Search Results: 1 in Date '2012-11'
Title / Author(s) / Keywords
Matrix Cracking Detection by Acoustic Emission in Polymer Composites and Counts/Duration ratio
C. Santulli20
Electrical Engineering Department; Università di Roma - La Sapienza31, Rome, Italy
Acoustic emission, matrix cracking, polymer composites, frequency, counts, duration, amplitude

   