where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -
Issue '2016-02'
Vol.21 No.02 - The e-Journal of Nondestructive Testing - ISSN 1435-4934
Summary

In this month issue we are publishing the proceedings of the Conference on Industrial Computed Tomography (iCT) 2016, 9-12 February 2016, Wels, Austria. It is the first time that we are publishing already before the conference its proceedings via the
...
database. By this service the participants can benefit by accessing the proceedings during the conference from different devices, the organizer have no needs to hand-out proceedings on CD or USB media and of course the whole NDT community can virtually take part on this conference. NDT.net can publish online proceedings just within a couple of dates from time of receiving the PDF and a table of content. Updates of late received papers, powerpoints, posters or movies are possible as another benefit of online proceedings.
56 Articles:6th Conference on Industrial Computed Tomography (iCT) 2016, 9-12 February 2016, Wels, Austria
iCT 2016 papers are for the first time already before the conference imported and available in NDT.net. By this service the conference participants can access the papers during the conference and of course the whole NDT community.

Call for Papers: EWGAE 2016

32st Conference of the European Working Group on Acoustic Emission, 2016 Sep 7-9, Prague, Czech Republic more

Simpleware Ltd

United Kingdom, Other

TESTIA

France, ET, MT, Other Methods, PT, RT, UT, VT/OT Consulting, Course Provider, Inspection

VJ Technologies

USA, Other Methods, RT Consulting, Inspection, Research

Silverwing

United Kingdom, Other Methods, UT Inspection, Manufacturer
New Events & Web Resources |more|
12 News in this issue
Dynamic IR Imaging
InfraTec GmbH
TSC exhibiting at Subsea Expo 2016, showcasing the MagCrawler
TSC Inspection Systems
Zetec’s New High Stability Bobbin Probe Can Deliver Increase of 30% or More in Probe Life
Zetec
Zetec QuartZ Ultrasonic Instrument Speeds Up Complex Inspections
Zetec
Report on thickness measurement of basis metal through paint and compound coatings using Ultrasonic Thickness Gauge А1210
Acoustic Control Systems Ltd.
TWI has launched two new corrosion detection courses
TWI Ltd (The Welding Institute)
Dolphitech and Sonatest announce distribution agreement
DolphiTech AS
Jireh Industries Expands to Larger Sales and Support Facility in Houston
Jireh Industries
Eddyfi Inaugurates Middle East Office in Abu Dhabi
Eddyfi
CIVA Newsletter January 2016
EXTENDE
Non Destructive Testing (NDT) Market by Method (UT, RT, LPT, MPT, ECT, VI), End-User (Aerospace & Defense, Power Generation, Infrastructure, Oil & Gas, Automotive), Technique, Application & Region (G7, BRICS, RoW) – Global Forecast to 2020
MarketsandMarkets
Global Non-Destructive Testing Equipment Market Outlook (2015-2022)
STRATISTICS MRC
Table of Contents
58 Articles in
Issue: 2016-02
Filter Results ...
Publications
iCT 2016 (56)
NDT.net Journal (2)
Exhibitors (4)
EXTENDE.. 1
Materials Rese.. 1
YXLON Internat.. 2
Title / Author(s) / Keywords Publication
Photoelastic Visualisation: Phased Array Sound Fields Part 22 – Phased array Tip Diffraction L-mode
E. Ginzel99
Materials Research Institute102, Waterloo, Canada
Ultrasonic Testing (UT), phased array, tip diffraction, ultrasonic, Photoelastic visualisation

/1
NDT.net Journal
Physical Integrity Verification of Submerged Structures with Laser Scanner
J. Balieiro, D. Oliveir
The Federal University of Pará (UFPA)4, Pará, Brazil
Visual and Optical Testing (VT/OT)

NDT.net Journal
iCT 2016 Algorithms, optimisations and visualisations
Efficient Iterative CT Reconstruction on Octree Guided by Geometric Errors
S. Kim1, A. Sakane1, Y. Ohtake118, H. Suzuki118, Y. Nagai113, K. Sato22, H. Fujimoto35, M. Abe36, O. Sato34, T. Takatsuji36
1School of Engineering; University of Tokyo65, Tokyo, Japan
2Hitachi Ltd4, Yokohama, Japan
3National Metrology Institute of Japan (NMIJ)4, Tsukuba, Japan
CT reconstruction, Adaptive data structure, Iterative algorithm, Geometric error driven method

iCT 2016
Session: Algorithms, optimisations and visualisations
iCT 2016 Algorithms, optimisations and visualisations
The MUSICES Project: Simulative automated CT acquisition planning for historical brass instruments improves image quality
R. Schielein1,28, G. Scholz27, C. Kretzer26, T. Fuchs226, S. Kasperl238, F. Bär36, S. Kirsch36, M. Zepf32, M. Wolters-Rosbach35
1X-ray Microscopy; Julius-Maximilians-University Würzburg13, Würzburg, Germany
2Development Center X-ray technology (EZRT); Fraunhofer Institute for Integrated Circuits (IIS)185, Fürth, Germany
3Germanisches Nationalmuseum (GNM)6, Nürnberg, Germany
X-Ray simulation, quantitative image characterization, computed tomography of cultural heritage, CT acquisition planning

iCT 2016
Session: Algorithms, optimisations and visualisations
iCT 2016 Algorithms, optimisations and visualisations
A novel Method for Determination of Fiber Length Distributions from µCT-data
P. Pinter, B. Bertram, K. Weidenmann2
Institute for Applied Materials; Karlsruhe Institute of Technology (KIT)5, Karlsruhe, Germany
Radiographic Testing (RT), fibre reinforced polymers, X-ray computed tomography, fibre length distribution, fiber tracking

iCT 2016
Session: Algorithms, optimisations and visualisations
iCT 2016 Manufacturing, NDT and instrumentation
Automatic Object Position Recognition: Increasing the Position-Accuracy in Robot-CT
P. Klein7, F. Herold28
YXLON International GmbH197, Hamburg, Germany
Computed Tomography, Robot-CT, Measurement Accuracy

iCT 2016
Session: Manufacturing, NDT and instrumentation
iCT 2016 Manufacturing, NDT and instrumentation
Investigation on Effect of scintillator thickness on image lag in Indirect- Flat Panel Detectors
K. Zarei zefreh12, J. De Beenhouwer117, F. Marone Welford22, J. Sijbers120
1iMinds-Visionlab; University of Antwerpen36, Antwerpen, Belgium
2X-ray Tomography Group; Swiss Light Source2, Villigen, Switzerland
x-ray detector, flat-panel, image lag, scintillator thickness, synchrotron

iCT 2016
Session: Manufacturing, NDT and instrumentation
iCT 2016 Manufacturing, NDT and instrumentation
Parametric design in Reverse Engineering based on CT data
D. Hofmann3, P. Sembdner3, S. Holtzhausen3, C. Schöne, R. Stelzer3
Department of Mechanical Engineering, Institute of Machine Elements and Machine Design; Dresden University of Technology (TU Dresden)80, Dresden, Germany
NDT-wide, CT data, Reverse Engineering, Parametric design

iCT 2016
Session: Manufacturing, NDT and instrumentation
iCT 2016 Manufacturing, NDT and instrumentation
CT-based quality control of Laser Sintering of Polymers
M. Pavan15, T. Craeghs16, J. Kruth212, W. Dewulf221
1R&D; Materialise NV6, Leuven, Belgium
2Department of Mechanical Engineering; Catholic University of Leuven (KU Leuven) 105, Leuven, Belgium
Radiographic Testing (RT), polymers, quality control, Computed Tomography, Non-destructive testing, Laser Sintering, porosity analysis, Scanning Strategy
iCT 2016
Session: Manufacturing, NDT and instrumentation
iCT 2016 Materials characterisation
Size and shape determination of sub-millimeter sized abrasive particles with X-ray computed tomography
C. Rothleitner, U. Neuschaefer-Rube13, J. Illemann8
Physikalisch-Technische Bundesanstalt (PTB)45, Braunschweig, Germany
Radiographic Testing (RT), Computed Tomography, 3D Analysis, X-ray, abrasive particles, particle characterization, Size and Shape of Particles

iCT 2016
Session: Materials characterisation
iCT 2016 Materials characterisation
3D microstructure and damage accumulation in a cast AlSi12Cu5Ni2-Mg piston alloy as a function of solution treatment
K. Bugelnig1, G. Requena211, F. Sket32, F. Wilde43
1Inst. of Materials Science & Technology; Vienna University of Technolog (TU)57, Vienna, Austria
2German Aerospace Center (DLR)8, Cologne, Germany
3Madrid Institute for Advanced Studies of Materials (IMDEA Materials Institute)4, Madrid, Spain
4Helmholtz-Zentrum Geesthacht8, Geesthacht, Germany
Other Methods, Synchrotron Tomography, Damage evolution, Al-Si piston alloys, solution treatment, 3D microstructure

iCT 2016
Session: Materials characterisation
iCT 2016 Materials characterisation
Digital Volume Correlation for Strain Mapping of Industrial Materials
N. Lippiatt, M. Wevers54
Department of Metallurgy and Materials Engineering (MTM); Catholic University of Leuven (KU Leuven) 105, Leuven, Belgium
Radiographic Testing (RT), image analysis, metrology, tomography

iCT 2016
Session: Materials characterisation
iCT 2016 Materials characterisation
Comparision of different segmentation methods for porosity evaluation in CFRP-reference samples and comparison with real porosity samples
G. Rao8, B. Plank49, J. Kastner123
R&D Competence Center; Upper Austrian University of Applied Sciences (FH OÖ)171, Wels, Austria
Radiographic Testing (RT), Other Methods, composite, materials characterization, porosity, carbon fiber reinforced plastic (CFRP), visualization, Computed Tomography, reference sample

iCT 2016
Session: Materials characterisation
iCT 2016 Materials characterisation
Comparison of predicted and measured fiber orientations in injection molded parts
G. Gsellmann1, M. Jerabek13, D. Salaberger239
1Borealis Polyolefine GmbH6, Linz, Austria
2R&D Competence Center; Upper Austrian University of Applied Sciences (FH OÖ)171, Wels, Austria
AMI 2016, Autodesk Moldflow, fiber orientation, computed tomography, Folgar-Tucker, residual strain closure

iCT 2016
Session: Materials characterisation
iCT 2016 Metrology
Quality evaluation of X-ray computed tomography volume data in dimensional metrology
L. Xue1, H. Suzuki118, Y. Ohtake118, H. Fujimoto25, M. Abe26, O. Sato24, T. Takatsuji26
1RCAST; University of Tokyo65, Tokyo, Japan
2National Metrology Institute of Japan (NMIJ)4, Tsukuba, Japan
X-ray computed tomography, dimensional metrology, image quality, measurement accuracy, entropy

iCT 2016
Session: Metrology
iCT 2016 Metrology
Numerical measurement uncertainty determination for dimensional measurements of microparts with CT
E. Helmecke14, M. Fleßner15, A. Staude228, T. Hausotte114
1Institute of Manufacturing Metrology; University of Erlangen-Nürnberg (FAU)45, Erlangen, Germany
2BAM Federal Institute for Materials Research and Testing1324, Berlin, Germany
computed tomography, dimensional metrology, standardization, numerical uncertainty determination, Virtual Metrological CT

iCT 2016
Session: Metrology
iCT 2016 Metrology
Development of test bodies for deployment in industrial Computed Tomography
A. Kraemer3, A. Batra, G. Lanza13
wbk Institute of Production Science; Karlsruhe Institute of Technology (KIT)22, Eggenstein, Germany
Radiographic Testing (RT), Other Methods, metrology, traceability, Computed Tomography, Geometric Tolerances

iCT 2016
Session: Metrology
iCT 2016 Metrology
Experimental assessment of computed tomography dimensional performance using modular test pieces made of polyoxymethylene and aluminum
C. Baldo17, T. Fernandes26, G. Donatelli211
1Modeling and Applied Social Sciences Center; Federal University of ABC (UFABC)7, Santo André, Brazil
2Center for Metrology and Instrumentation; CERTI Foundation12, Florianópolis, Brazil
computed tomography, measurement uncertainty, features of size, modular test artefacts

iCT 2016
Session: Metrology
iCT 2016 Metrology
Novel evaluation method of low contrast resolution performance of dimensional X-ray CT
M. Abe6, H. Fujimoto5, O. Sato4, K. Matsuzaki2, T. Takatsuji6
National Metrology Institute of Japan (NMIJ)4, Tsukuba, Japan
dimensional metrology, X-ray computed tomography, contrast, resolution

iCT 2016
Session: Metrology
iCT 2016 Metrology
Assessment of the single point uncertainty of dimensional CT measurements
M. Fleßner5, A. Müller10, D. Götz, E. Helmecke4, T. Hausotte14
Institute of Manufacturing Metrology; University of Erlangen-Nürnberg (FAU)45, Erlangen, Germany
computed tomography, dimensional metrology, single point uncertainty, measurement uncertainty, error sources

iCT 2016
Session: Metrology
 
Page:
 -1-   2   3 
next pageNext
Actual Cooperations
Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window