Summary
2 Articles:Journal of Acoustic Emission (ISSN 0730-0050), Published by Acoustic Emission Group, Encino, CA, USA
Editor: Kanji Ono, Associate Editors: A. G. Beattie, T. F. Drouillard, M. Ohtsu and W. H. Prosser. Acoustic Emission Working Group (AEWG), European Working Group on Acoustic Emission (EWGAE), have endorsed the publication of Journal of Acoustic Emission.
...
Journal of Acoustic Emission is published annually in CD-ROM by Acoustic Emission Group, PMB 409, 4924 Balboa Blvd, Encino, California 91316 (USA). It may also be reached at 2121H, Engr. V, University of California, Los Angeles, California 90095-1595 (USA). Tel. +1 (310) 825-5233. Fax +1 (310) 206-7353. e-mail: aegroup7@gmail.com or ono@ucla.edu.
>

NDT.net at the WCNDT 2016 June 12-17

Rolf Diederichs presents

Call for Papers: AeroNDT 2016

8th International Symposium on NDT in Aerospace, 2016 Nov 3-5, Bangalore, India

Call for Papers: iCT 2017

7th Conference on Industrial Computed Tomography, Feb 7-9 2017, Leuven, Belgium

NDT Days 2016

International Conference NDT Days 2016, June 6 - 11, Sozopol, Bulgaria

NextNDT Technology, Inc.

USA, OtET, RT, UT, Manufacturer
New Events & Web Resources |more|
15 News in this issue
Sonotron NDT introduces the VAUT technology
Sonotron NDT
YXLON International is proud to announce the latest technology advances to their market leading FeinFocus product range for electronics applications
YXLON International GmbH
Announcing the Launch of Magnifi SR and Magnifi GO 1.1
Eddyfi
New Ultrasonic Inspection Systems Developed by Eurosonic Mistras
Eurosonic Mistras
Ultrasonic Manual High-Temperatures Scanner
Eurosonic Mistras
Jireh Industries Releases New Pit Depth Inspection Tool
Jireh Industries
Volume Graphics Releases VGStudio MAX 3.0
Volume Graphics GmbH
Jireh Industries Releases Reduced Width Chain Scanner
Jireh Industries
The Pixel Millionaire
InfraTec GmbH
GE Brings Digital Solutions to Nondestructive Testing (NDT) Industry
GE Inspection Technologies GmbH
Acoustic Control Systems Ltd. has been completing modernization of electro-magnetic acoustic thickness gauge A1270 with innovative electro - magnetic biasing technology
Acoustic Control Systems Ltd.
NDT Inspection Techniques for A340 Rudder Assessment Thermography and Elch
TESTIA France
TECNATOM’S Robotic Systems at JEC World 2016: The Latest Technology For Aero‐parts Non Destructive Inspection
Tecnatom S.A.
Annual Report 2015 now online
Fraunhofer-Institute for Non-Destructive Testing (IZFP)
First announcement for the 14th Int. Conference titled “Application of Contemporary Non-destructive Testing in Engineering”
Slovenian Society for Non-destructive Testing
Table of Contents
23 Articles in
Issue: 2016-05
Filter Results ...
Publications
NDT Review (11)
NDT.net Journal (7)
AeroNDT 2015 (3)
Journal-AE (2)
Exhibitors (3)
Innovation Pol.. 1
Materials Rese.. 2
Title / Author(s) / Keywords Publication
Low Velocity Elastomer Polymer Wedges Applied to TOFD
E. Ginzel196, R. Ginzel222, R. MacNeil24
1Materials Research Institute99, Waterloo, Canada
2Innovation Polymers6, Kitchener, Ontario, Canada
TOFD, polymers, velocity, ultrasonic

NDT.net Journal
Acoustic Velocity Determination for AUT on Spiral Pipe Girth Welds
E. Ginzel196, H. Van Dijk23
1Materials Research Institute99, Waterloo, Canada
2JES Pipelines, Willemstad, Canada
Ultrasonic Testing (UT)

NDT.net Journal
Development of NDT Based Electronic System for measurement of ultrasonic Parameter of Coal Sample
D. Kate, N. Choudhari2, A. Choudhari
Department of Electronics and Communication; Bhagwati College of Engineering2, Nagpur, India
Ultrasonic, Coal, NDT, Velocity, attenuation

NDT.net Journal
An Overview Algorithm to Minimise Side Lobes for 2D Circular Phased Array
S. Mondal
School of Engineering; London South Bank University6, London, United Kingdom
Phased array, ultrasonic beam focusing and total focusing method

NDT.net Journal
Impact-Echo Technique to Assess Concrete Structures
R. Otero19, G. Sulbarán22, E. Moreno37
1Centro de Tecnología de Materiales; Fundación Instituto de Ingeniería3, Caracas, Venezuela
2Ingenieros Asesores en Metalurgia y Soldadura, , Mexico
3Technological Centre; Fundacion Tecnalia R&I5, Minano, Spain
Ultrasonic Testing (UT)

NDT.net Journal
The Ultrasonic Polar Scan for Composite Characterization and Damage Assessment: Past, Present and Future
M. Kersemans17, A. Martens22, J. Degrieck18, K. Van den Abeel28, S. Delrue27, L. Pyl36, F. Zastavnik34, H. Sol35, W. Van Paepegem17
1Department of Materials Science and Engineering; University of Ghent (UGent)51, Ghent, Belgium
2aDepartment of Materials Science and Engineering bWave Propagation and Signal Processing Group; Katholieke Universiteit Leuven Campus Kulak (KULK) 13, Kortrijk, Belgium
3Department Mechanics of Materials and Constuctions; Vrije Universiteit Brussel (VUB) 54, Brussel, Belgium
ultrasound, ultrasonic polar scan, composites, NDT, characterization, damage

NDT.net Journal
Lamb Wave Interaction with Adhesively Bonded Stiffeners and Disbonds Using 3D Vibrometry
R. Marks1, A. Clarke12, C. Featherston16, C. Paget22, R. Pullin119
1School of Engineering; Cardiff University25, Cardiff, United Kingdom
2Airbus Operations4, Bristol, United Kingdom
lamb waves, vibrometry, adhesive bonding, ultrasonics, non-destructive testing, structural health monitoring

NDT.net Journal
Journal-AE Volume 32, 2014
Acquisition of Complete Acoustic Emission Amplitude Records during Rock Fracture Experiments
S. Goodfellow1, J. Flynn2, J. Reyes-montes2, M. Nasseri1, R. Young12
1Department of Civil Engineering; University of Toronto40, Toronto, Canada
2Applied Seismology Consultants, Shrewsbury, United Kingdom

Journal-AE
Session: Volume 32, 2014
Journal-AE Volume 32, 2014
Quantitative Evaluation of Rejuvenators to Restore Embrittlement Temperatures in Oxidized Asphalt Mixtures using Acoustic Emission
Z. Sun, N. Farace, B. Behnia2, W. Buttlar3, H. Reis4
aDepartment of Industrial and Enterprise Systems Engineering bDepartment of Civil and Environmental Engineering; University of Illinois14, Urbana, IL,, USA
Asphalt concrete, oven-aging, embrittlement temperatures, asphalt binder, rejuvenator

Journal-AE
Session: Volume 32, 2014
AeroNDT 2015 Emerging Technology in Electromagnetism
Diagnostics of Degradative Changes in Paramagnetic Alloys with the use of Low Frequency Impedance Spectroscopy
Z. Żurek19, M. Witoś215
1Silesian University of Technology9, Katowice, Poland
2Air Force Institute of Technology34, Warsaw, Poland

AeroNDT 2015
Session: Emerging Technology in Electromagnetism
AeroNDT 2015 IT Developments and Solutions
IT Support of NDE and SHM with Application of the Metal Magnetic Memory Method
M. Witoś15, M. Zieja4, B. Kurzyk2
Air Force Institute of Technology34, Warsaw, Poland

AeroNDT 2015
Session: IT Developments and Solutions
AeroNDT 2015 Structural Health Monitoring in General
Expert System to Support Operational Safety of the TS-11“Iskra” Aircraft and Overhauls of the SO-3 Engines
M. Witoś15, M. Wachłaczenko5
Air Force Institute of Technology34, Warsaw, Poland

AeroNDT 2015
Session: Structural Health Monitoring in General
NDT Review Materials (MDPI)
Internal Stress Monitoring of In-Service Structural Steel Members with Ultrasonic Method
Z. Li14, J. He14, J. Teng15, Y. Wang24
1School of Civil and Environment Engineering, Shenzhen Graduate School; Harbin Institute of Technology (HIT)38, Harbin, China
2Department of Civil and Environmental Engineering; University of Surrey10, Surrey, United Kingdom
Ultrasonic Testing (UT), acoustoelasticity, Internal stresses, longitudinal critically refracted waves

NDT Review
Session: Materials (MDPI)
NDT Review Sensors (MDPI)
High Temperature Shear Horizontal Electromagnetic Acoustic Transducer for GuidedWave Inspection
M. Kogia, T. Gan30, W. Balachandran6, M. Livadas3, V. Kappatos10, I. Szabo, A. Mohimi3, A. Round
Brunel Innovation Centre ((BIC); Brunel University36, Uxbridge, United Kingdom
Electromagnetic Acoustic Transducers, EMAT, Guided Wave Testing, high temperature inspection

NDT Review
Session: Sensors (MDPI)
NDT Review Sensors (MDPI)
A Practical and Portable Solids-State Electronic Terahertz Imaging System
K. Smart1, J. Du1, L. Li1, D. Wang1, K. Leslie1, F. Ji2, D. Zeng2, X. Li2
1Commonwealth Scientific and Industrial Research Organisation (CSIRO)2, Lindfield, Australia
2Chengdu Shuguang Optical Fiber Network Co., Ltd, Chengdu, China
terahertz, imaging, solid-state electronic components

NDT Review
Session: Sensors (MDPI)
NDT Review Sensors (MDPI)
Dynamic Measurement for the Diameter of A Train Wheel Based on Structured-Light Vision
Z. Gong, J. Sun, G. Zhang
Key Laboratory of Precision Opto-Mechatronics Technology, Ministry of Education; Beihang University (BUAA)39, Beijing, China
train wheel diameter, dynamic measurement, structured-light vision, machine vision

NDT Review
Session: Sensors (MDPI)
NDT Review Sensors (MDPI)
Reducing Sweeping Frequencies in Microwave NDT Employing Machine Learning Feature Selection
A. Moomen1, A. Ali22, O. Ramahi22
1Department of Computer Science; Rochester Institute of Technology, Rochester, USA
2Electrical and Computer Engineering (ECE); University of Waterloo18, Waterloo, Canada
microwave sensors, nondestructive testing, feature selection, machine learning

NDT Review
Session: Sensors (MDPI)
NDT Review Sensors (MDPI)
Concrete Condition Assessment Using Impact-Echo Method and Extreme Learning Machines
J. Zhang1, Y. Weizhong2, D. Cui1
1Anhui and Huaihe River Institute of Hydraulic Research, Bengbo,
2GE Global Research4, Niskayuna, NY, USA
defect detection, extreme learning machine, feature extraction, machine learning, nondestructive testing, wavelet transform

NDT Review
Session: Sensors (MDPI)
NDT Review Sensors (MDPI)
Evaluation of SHM System Produced by Additive Manufacturing via Acoustic Emission and Other NDT Methods
M. Strantza5, D. Aggelis27, D. De Baere6, P. Guillaume11, D. Van Hemelrijck18
aDepartment of Mechanics of Materials and Constructions b2Department of Mechanical Engineering and Aeronautics cDepartment of Mechanical Engineering cDepartment Mechanics of Materials & Constructions (MeMC; Vrije Universiteit Brussel (VUB) 54, Brussel, Belgium
acoustic emission, additive manufacturing, structural health monitoring, liquid penetrant inspection, radiography, eddy current

NDT Review
Session: Sensors (MDPI)
NDT Review Sensors (MDPI)
A Micro-Computed Tomography Technique to Study the Quality of Fibre Optics Embedded in Composite Materials
G. Chiesura1, G. Luyckx15, E. Voet12, N. Lammens13, W. Van Paepegem17, J. Degrieck18, M. Dierick14, L. Van hoorebeke16, P. Vanderniepen1, S. Sulejmani24, C. Sonnenfeld23, T. Geernaert26, F. Berghmans26
1aDepartment of Materials Science and Engineering bDept. Physics and Astronomy; University of Ghent (UGent)51, Ghent, Belgium
2Brussels Photonics Team (B-PHOT); Vrije Universiteit Brussel (VUB) 54, Brussel, Belgium
carbon fibre, defects, radiography, autoclave, prepreg

NDT Review
Session: Sensors (MDPI)
 
Page:
 -1-   2 
next pageNext
Actual Cooperations
Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window