where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -
Issue '2016-11'
Vol.21 No.11 - The e-Journal of Nondestructive Testing - ISSN 1435-4934
Summary

APCNDT 2017 Nov 13-17, Singapore

Asia Pacific Conference on Non-Destructive Testing (15th APCNDT), Abstract submission is now open

Laser Optical Engineering Ltd

Other Methods, VT/OT Inspection, United Kingdom, Manufacturer
New Events & Web Resources |more|
14 News in this issue
Phased array inspection (PAUT) of complex geometry welds with use of ISONIC series instruments from Sonotron NDT
Sonotron NDT
Eddyfi Launches Tank Floor Pulsed Eddy Current (PEC) Probe
Eddyfi
Teledyne DALSA Launches Portable Digital Radiography System at ASNT Annual Conference
Teledyne DALSA
Tecnatom’s Technology Contributes to Increase Productivity
Tecnatom S.A.
Compensator factory near Esbjerg
YXLON International AS
The National Gallery of Denmark
YXLON International AS
New World Class Products Emerge From Global Partnership; Inspection Prowess, Automation Leadership, Innovative Research & Development
VJ Technologies
TSC are proud to announce a new European distributor partnership
TSC Inspection Systems
Fraunhofer IZFP receives an order worth half a million euros in the Persian Gulf
Fraunhofer-Institute for Non-Destructive Testing (IZFP)
Creaform and Sonatest announce a new global distribution partnership
Sonatest Ltd
FORCE Technology Wins Asset Integrity Management Contract with BP Norway
FORCE Technology
Non Destructive Testing of defects in oil and gas pipelines
Brunel University
Sandvik inaugurates new, fully automated OCTG ultrasonic testing facility
Sandvik AB
ZfP Zeitung Ausgabe 151
Deutsche Gesellschaft für Zerstörungsfreie Prüfung (DGZfP)
Table of Contents
64 Articles in
Issue: 2016-11
Filter Results ...
Publications
EWGAE 2016 (62)
NDT.net Journal (2)
Exhibitors (5)
Materials Rese.. 1
Ultrasound Ins.. 1
Vallen-Systeme.. 3
Title / Author(s) / Keywords Publication
Photoelastic Visualisation of Phased Array Sound Fields: Part 23 – The So-Called Creeping Wave – Near Surface
E. Ginzel99
Materials Research Institute102, Waterloo, Canada
Photoelastic visualisation, ultrasonic, Creeping Wave
/1
NDT.net Journal
Control of ultrasound propagation through 3D-printed printed CFRP based on the curvature of the fibers
T. Ashizawa12, D. López-Rodrigo2, Y. Mizutani130
1Department of Mechanical Engineering; Tokyo Institute of Technology45, Tokyo, Japan
2School of Aeronautics and Space Engineering; Technical University of Madrid (UPM) 54, Madrid, Spain
Ultrasound addressing, 3D-printing, carbon fiber-reinforced plastic (CFRP), orthotropic materials, attenuation

NDT.net Journal
EWGAE 2016 undefined
Monitoring of Deep Groove Ball Bearing Defects Using the Acoustic Emission Technology
M. El-shaib3, O. Keshk, M. Sheheda2
Arab Academy for Science Technology & maritime Transport (AASTMT)8, Alexandria, Egypt
Acoustic emission, bearing defect diagnosis, condition monitoring

EWGAE 2016
Session: undefined
EWGAE 2016 undefined
Seeded Fault Detection on Spur Gears with Acoustic Emission
M. El-shaib3, O. Hammoda, M. Sheheda2
Arab Academy for Science Technology & maritime Transport (AASTMT)8, Alexandria, Egypt
Acoustic Emission (AE), condition monitoring, Acoustic emission, spur gear, Seed Fault

EWGAE 2016
Session: undefined
EWGAE 2016 Advanced Composites
Influence of Attenuation on the Acoustic Emission B-Value for Damage Evaluation of Reinforced Concrete Specimens
F. Sagasta13, Y. Mizutani230, I. Valverde1, E. Suarez17, F. Rescalvo14, A. Gallego130
1aDepartment of Applied Physics bDepartment of Building Constructions cSchool of Engineering Building; University of Granada34, Granada, Spain
2Department of Mechanical Sciences and Engineering; Tokyo Institute of Technology45, Tokyo, Japan
acoustic emission, attenuation, b-value, macroscopic-fracture, damage evaluation, reinforced concrete

EWGAE 2016
Session: Advanced Composites
EWGAE 2016 Advanced Composites
Detecting the Critical Strain of Fiber Reinforced Plastics by Means of Acoustic Emission Analysis
F. Willems3, J. Benz2, C. Bonten3
Institut für Kunststofftechnik; University of Stuttgart285, Stuttgart , Germany
Acoustic Emission (AE), micro cracks, Tensile test, acoustic emission analysis, critical strain, failure limit, engineering design, fiber reinforced plastics

EWGAE 2016
Session: Advanced Composites
EWGAE 2016 Advanced Composites
Acoustic Emission Testing of Composite-to-Metal and Metal-to-Metal Adhesive Bond Strengths
M. Droubi15, N. Faisal14, A. Stuart1, J. Mowat12, C. Nobel1, M. El-shaib23
1School of Engineering; Robert Gordon University8, Aberdeen, United Kingdom
2Marine Engineering Department; Arab Academy for Science Technology & maritime Transport (AASTMT)8, Alexandria, Egypt
Acoustic Emission (AE), failure mode, adhesive bond strength.

EWGAE 2016
Session: Advanced Composites
EWGAE 2016 Advanced Composites
Damage Type Identication Based on Acoustic Emission Detection Using a Fiber-Optic Sensor in Carbon Fiber Reinforced Plasitc Laminates
F. Yu15, Y. Okabe19, Q. Wu14, N. Shigeta2
1Institute of Industrial Science; University of Tokyo65, Tokyo, Japan
2Institute of Industrial Science; IHI Corporation, Tokyo, Israel
Optical Fiber Sensor, Composite Material, Guided Wave

EWGAE 2016
Session: Advanced Composites
EWGAE 2016 Advanced Composites
Change in b-value by AE Propagation Length in CFRP
D. JUNG, Y. Mizutani30, A. Todoroki18, Y. Suzuki9
Tokyo Institute of Technology45, Tokyo, Japan
b-value, Carbon Fiber Reinforced Plastic(FRP), Frequency dependence of Attenuation

EWGAE 2016
Session: Advanced Composites
EWGAE 2016 Advanced Composites
Development of a method for classifying CFRP fracture modes by AE testing
Y. Hata, Y. Mizutani30, A. Todoroki18, Y. Suzuki9
Tokyo Institute of Technology45, Tokyo, Japan
Acoustic Emission (AE), signal processing, Wavelet transform, Lamb wave, Carbon Fibre Reinforced Plastic, Fracture Mode Classification, All Pass Function, Phase Shift Function

EWGAE 2016
Session: Advanced Composites
EWGAE 2016 Advanced Composites
Manual Lamb Wave Tomography Utilizing AE Technique
Y. Mizutani30, T. Miki, A. Todoroki18, Y. Suzuki9
Department of Mechanical Sciences and Engineering; Tokyo Institute of Technology45, Tokyo, Japan
Lamb wave, Tomography, thin structures, anisotropy, source location, carbon fibre composite

EWGAE 2016
Session: Advanced Composites
EWGAE 2016 Advanced Composites
Measurement of Electromagnetic Emission As a Tool to Study Fracture Processes of Carbon Fibre Reinforced Polymers
S. Gade5, P. Potstada3, B. Alaca2, M. Sause43
Institute for Physics, Experimentalphysik; University of Augsburg44, Augsburg, Germany
electromagnetic emission, acoustic emission, fibre reinforced polymers, fracture mechanics

EWGAE 2016
Session: Advanced Composites
EWGAE 2016 Advanced Composites
Pattern Recognitionof Acoustic Emissionsignal Duringthe Mode I Fracture Mechanismsin Carbon- Epoxy Composite
N. Fallahi12, G. Nardoni134, R. Palazzetti2, A. Zucchelli3
1I&T Nardoni Institute35, Brescia, Italy
2DMEM department; University of Strathclyde33, Glasgow, Scotland, United Kingdom
3DIN department; University of Bologna52, Bologna, Italy
Acoustic Emission (AE), Carbon epoxy composites, failure mechanisms, self organizing map, learning vector quantization (LVQ)

EWGAE 2016
Session: Advanced Composites
EWGAE 2016 Advanced Composites
Acoustic Emission Source Identification in Large Scale Fibre Reinforced Composites
M. Sause43
Institute for Physics; University of Augsburg44, Augsburg, Germany
source identification, fibre reinforced composites, acoustic emission

EWGAE 2016
Session: Advanced Composites
EWGAE 2016 Advanced Composites
Correlation Between Acoustic Emission Signals And Delaminations in Carbon Fiber-Reinforced Polymer-Matrix Composites: A New Look at Mode I Fracture Test Data
A. Brunner26
Laboratory for Mechanical Systems Engineering; Empa, Swiss Federal Laboratories for Materials Science and Technology96, Dübendorf, Switzerland
Carbon fiber-reinforced polymer-matrix composites, mode I tensile-opening fracture, measurement sensitivity, acoustic emission intensity correlation

EWGAE 2016
Session: Advanced Composites
EWGAE 2016 Advanced Composites
Acoustic Emission Comparative Study of Carbon/Epoxy Composites under Load
B. Muravin15, T. Gottesman2
1Integrity Diagnostics Ltd.3, Netanya, Israel
2Israel Ministry of Defense, Tel Aviv, Israel
Acoustic emission, carbon fiber laminates, damage accumulation

EWGAE 2016
Session: Advanced Composites
EWGAE 2016 AE in Different Applications
Monitoring Industrial Crystallization using Acoustic Emission
E. Serris3, A. Cameirao, F. Gruy
Ecole Nationale Supérieure des Mines de Saint-Etienne3, Saint-Etienne, France
particle size, crystallisation, monitoring, industrial processes

EWGAE 2016
Session: AE in Different Applications
EWGAE 2016 AE in Different Applications
Two-Dimensional Q-Value AE-Tomography and its Verification on Numerical Invesitigations
Y. Kobayashi15, T. Shiotani229
1College of Science and Technology; Nihon University9, Tokyo, Japan
2Graduate School of Engineering/ Graduate School of Business; Kyoto University33, Kyoto, Japan
AE-Tomography, Q-Value distribution

EWGAE 2016
Session: AE in Different Applications
EWGAE 2016 AE Signal Processing and Source Location
Obtaining Wave-Path Information from pulsed Sensor Pairs
H. Vallen39, T. Thenikl18, H. Trattnig7
Vallen-Systeme GmbH47, Icking, Germany
Acousto-Ultrasonics, pulsed-AE, AE-wave-paths

EWGAE 2016
Session: AE Signal Processing and Source Location
EWGAE 2016 AE Signal Processing and Source Location
From Near Field to Far Field and Beyond
M. šofer1, J. Crha24, H. Zengerle3
1Department of Applied Mechanics; VSB-Technical University of Ostrava11, OSTRAVA, Czech Republic
2AE CONSULTANT4, OSTRAVA, Czech Republic
3Department of Mechanical Engineering; Boston University6, Boston, MA, USA
Acoustic Emission (AE), reflection, Dispersion, absorption, near field, dissipation, Refraction, Far field, Attenuation curve

EWGAE 2016
Session: AE Signal Processing and Source Location
 
Page:
 -1-   2   3   4 
next pageNext
Actual Cooperations
Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window