Olympus Introduces the BTX Profiler, a Combined XRD-XRF Analyzer for Comprehensive Materials Analysis


Olympus Scientific Solutions Americas (OSSA)221, Waltham, MA, USA
 
NDT.net Journal
Issue: 2013-07
(Waltham, MA, USA - June 10, 2013) Olympus is pleased to announce the release of a new benchtop analyzer that combines X-ray Diffraction (XRD) and X-ray Fluorescence (XRF) in one unit. The BTX Profiler carries on the revolutionary XRD technology employed in NASA’s “Curiosity” Rover, part of the successful NASA Mars Science Laboratory program, and the highly acclaimed, award winning earthbound technology employed in Olympus Analytical X-ray Instruments. The BTX Profiler combines these to provide compositional materials analysis at the structural and elemental level affording economy of operational costs, space, and time with a seamless integration of data and results.

The BTX Profiler reduces inefficiencies found in conventional powder diffraction systems. Its close-coupled transmission geometry allows for a low powered X-ray source and a small amount of sample. The sophisticated sample handling technology incorporates a patented vibration system that enables random crystal orientation in a fixed sample cell. The CCD detector with its “smart” energy discrimination provides graphical 2-D diffraction patterns, or Ring Patterns, and acquires more data more quickly than conventional XRD detectors.

The Energy Dispersive XRF technology in the BTX Profiler integrates selectable optimized beam paths of a miniature X-ray tube and specialized filters, a large area silicon drift detector (SDD) for optimized resolution and detection limits, and close coupled geometry with the sample, allowing for a wide elemental and concentration measurement range.

The combination of all of these features reduces operational costs, space, and time of measurement while providing rapid, accurate and precise data analysis. The BTX Profiler’s nondestructive capability is of particular significance for several industrial sectors including energy, geochemistry, pharmaceuticals, catalysts, forensics and education.

For more information on the BTX Profiler, please visit http://www.olympus-ims.com/en/btx-profiler/.

About Olympus NDT
Olympus NDT is a world-leading manufacturer of innovative nondestructive testing instruments that are used in industrial and research applications ranging from aerospace, power generation, petrochemical, civil infrastructure, and automotive to consumer products. Leading-edge testing technologies include ultrasound, ultrasound phased array, eddy current, eddy current array and X-ray fluorescence. The Olympus NDT product lineup includes flaw detectors, thickness gages, in-line systems, automated systems, industrial scanners, analyzers, pulser-receivers, probes, transducers, and various accessories. Olympus NDT is also a distributor of remote visual inspection instruments and high-speed video cameras in the Americas. Olympus NDT is based in Waltham, Massachusetts, USA, and has sales and service centers in all principal industrial locations worldwide.

For more information please contact:
Kim Russell
Marketing Director
Analytical Instruments
(1) 781-419-4643
kim.russell@olympusNDT.com
Web: www.olympus-ims.com

Olympus Scientific Solutions Americas (OSSA)

More of Olympus Scientific Solutions Americas (OSSA) published in NDT.net
2019-05-01: 3 Tips for Accurate Small-Diameter Tubing Measurements
2019-04-01: Case Study: Inspecting Boiler Tube Welds Using the COBRA Ultrasonic Phased Array Solution Instead of Radiography
2019-04-01: Touch Down: Eddy Current Wheel Probes Help Ensure a Safe Landing
2019-03-01: Olympus Launches New Industrial Research Chair at Quebec Engineering School
2019-03-01: Eddy Current Array for Aircraft Engine Component Inspection
2019-03-01: Coherent Adaptive Focusing Technology for the Inspection of Variable Geometry Composite Material
2019-02-01: The (Sono)pen Is Mightier: 3 Tips to Improve Your Measurements
2019-01-01: For Goodness Sake - Assuring the Quality of Toys with Thickness Gages
2018-12-01: Train Inspection That Goes Beyond the Standard
2018-11-01: The FlexoFORM™ Scanner Provides a Complete Ultrasonic Testing Solution for Corrosion Inspection of Pipe Elbows
All 267 Articles & News of Olympus Scientific Solutions Americas (OSSA) in NDT.net

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window