TestPEP project success in developing new techniques for inspection of plastic pipes

TWI Ltd (The Welding Institute)183, Great Abington, Cambridge, United Kingdom

Webinars demonstrate the success of TestPEP

17 June 2013 . The TestPEP project team is pleased to announce the results of this EU-funded project to develop phased array inspection techniques for both butt fusion and EF welds in PE pipes for diameters 180-710 mm. The project conclusions, including a video demonstration of the new system, are being made available to view as a short series of webinars.

Plastic pipes have many advantages over pipes made from metals or concrete, such as good chemical resistance, low weight, low cost, and longer predicted service life, and are already used extensively for the transport of gas, water and chemicals. However their use in safety critical applications has been restricted by the lack of a validated inspection system being available to evaluate the joints.

Under the three-year project, the team designed and manufactured a prototype inspection system specifically for inspecting welded joints in PE pipes. This system has been assessed both in the laboratory/factory and in the field. Trials carried out on samples containing both real and artificial defects have proved successful in producing excellent results for butt fusion and EF welded joints.

The project consortium subsequently held four dissemination seminars to publicise the results of the project and these are available to view in the form of a webinar.

For further information please see the TestPEP website or email us.

The TestPEP project and website is managed by TWI and has received funding from the European Community's Seventh Framework Programme managed by REA-Research Executive Agency (FP7-SME-2008-2) under grant agreement no. 243791. Information is provided as is and no guarantee or warranty is given that the information is fit for any particular purpose. The user thereof uses the information at its sole risk and liability.

 
Visit: TWI Ltd (The Welding Institute)

Feedback: ()

Share:
More from "TWI Ltd (The Welding Institute)" (5 of 184)
2019-06-01OPTRAIL - Risk-Based Inspection for Optimised Maintenance
2019-05-01Digital Radiography Inspection of Flexible Risers in Offshore Oil and Gas Industry
2019-05-01NDT-In Service Inspection; Training and certification aspects
2019-04-01High Temperature Performance of Ultrasonic Guided Wave System for Structural Health Monitoring of Pipeline
2019-04-01Similarity Analysis Approach for Vibration Based Monitoring: An Application on a Train Door Mechanism
... All 184 Details >

More Videos in NDT.net

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window