Real-time auto-focussing through complex geometries components with full matrix capture


TWI Ltd (The Welding Institute)182, Great Abington, Cambridge, United Kingdom
 
NDT.net Journal
Issue: 2014-12
Case Study

Full matrix capture (FMC) imaging through a non-planar surface is a time-intensive task, due to the need to calculate the time of flight from each transmit/receive element combination to a given pixel in the region of interest through the refractive boundary. Due to the computational complexity, data is often post-processed after the inspection. TWI Technology Centre (Wales) has developed a real-time FMC imaging system capable of generating full-focused imagery through a component of complex geometry where no prior knowledge of the profile is provided.

Leading innovation in non-destructive testing

FMC is a relatively new ultrasonic non-destructive testing (NDT) technique, used to image sub-surface flaws in test components. The main advantage of FMC over existing phased array techniques is its ability to generate fully focused imagery of components. It achieves this by firstly acquiring the full time-domain signal for every possible transmit/receive combination, and then discretising the region of interest into a finite grid. Every cell in the grid is treated as a focal point and represents a pixel in the final image.

This ability to acquire the full time-domain signal from every possible transmit/receive element allows for changes in focal requirements to be determined dynamically and after acquisition, as there is no ultrasonic focusing within the component (as in the case of phased array).

Achievements

This work developed algorithms which:
generate fully focused imagery in real-time during the inspection from FMC data ultrasonically recognise and account for refractive boundaries between the ultrasonic transceiver and region of interest, to facilitate automated focusing and inspection through such boundaries offer a dynamic computationally efficient focal law calculator for systems containing refractive boundaries where the profile has not been provided produce high-quality imagery of components, allowing a more accurate assessment of flaw morphology and potentially improving the reliability of fitness-for-service evaluations.

Techniques involved

The ultrasonic and signal processing techniques developed were:
Acquisition of ultrasonic signals using the FMC technique
Real-time surface mapping of components using the FMC acquired data
Real time focal law updates to accommodate changes in surface profile.
Signal processing methods to calculate beam paths through refractive boundaries.

Experimental setup

To illustrate the effectiveness of the technique a part was manufactured with a profile of complex geometry, with which the FMC imaging system was provided with no prior knowledge. This component is shown in Figure 1. Custom FMC software was developed where the FMC imaging algorithm was used to image the component before and after accounting for the boundary. These results are shown in Figure 2.


Figure 1 Component of complex geometry


Figure 2 FMC imaging (left) before accounting for boundary and (right) after dynamically accounting for boundary in real-time

Future potential

The technique shows promise to deliver fast and accurate defect detection and characterisation, beyond what is currently achievable. Future work includes extending the capabilities of current auto-focus algorithms; converting algorithms for commercial application; and developing a robust, portable hardware system for on-site inspection.

TWI Ltd (The Welding Institute)

More of TWI Ltd (The Welding Institute) published in NDT.net
2019-05-01: Digital Radiography Inspection of Flexible Risers in Offshore Oil and Gas Industry
2019-05-01: NDT-In Service Inspection; Training and certification aspects
2019-04-01: High Temperature Performance of Ultrasonic Guided Wave System for Structural Health Monitoring of Pipeline
2019-04-01: Similarity Analysis Approach for Vibration Based Monitoring: An Application on a Train Door Mechanism
2019-01-01: Innovation in Robotic Inspection for Complex Geometries
2019-01-01: TWI JIP: Integrity of Mooring Chains using Acoustic Emission
2018-12-01: Enhancement of ultrasonic guided wave signals using split-spectrum processing technique
2018-11-01: Piezoelectric transducer excitation for guided waves propagation on pipeline with flexural wave modes
2018-11-01: A random vibration based platform for statistical damage detection in a population of nominally identical composite aerostructures
2018-11-01: Comparison of coded excitations in the presence of transducer’s transfer function in ultrasonic guided waves testing of pipelines
All 184 Articles & News of TWI Ltd (The Welding Institute) in NDT.net

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window