Introducing the multiple-angle TOFD wedge


Innovation Polymers6, Kitchener, Ontario, Canada
 
NDT.net Journal
Issue: 2018-11
High Density Poly Ethylene (HDPE) pipe is becoming a popular substitute for steel pipe. Varieties of polyethylene used in industry can have an acoustic velocity range from about 2100m/s to about 2600m/s. Using PMMA or polystyrene as a refracting wedge material could result in very little refraction or even negative refraction. Elastomeric materials designed by Innovation Polymers range from approximately 1025m/s to about 1600m/s, ensuring positive refraction for all applications on polyethylene.

Innovation Polymers has designed wedges specifically for TOFD applications on HDPE. Interchangeable plugs made from Innovation Polymers’ low velocity elastomeric polymers permits the user to select a refracted-angle option best suited for the TOFD inspection at hand. These wedges are primarily intended for the TOFD inspection of high density polyethylene butt fusion joints. The modular concept consists of a standard housing, replaceable plug inserts and a threaded plate to accommodate different sized probes up to 12.5mm (0.5 inch) diameter.

  • Standard plates are anodized aluminium with either 3/8-32 or 11/16-24 threaded opening for probes.
  • Standard incident angle is 35° on a flat contact surface.
  • Standard plugs are available in ACETM, AqualeneTM, and AqualinkTM.

    The standard materials provide refracted angles based on the polymer tested. User determines the best plug material, based on the polymer tested, its thickness, and the Probe Centre Spacing (PCS) for the desired depth of the beam crossing point.

    The flat wedge design with the soft polymer plugs allows the wedge to form to radii as low as 3” OD. Radiused wedges are available as a special order.

    Supplied with irrigation nozzles. Custom modifications can be made to accommodate different incident angles for the holder, different size of threaded probe-plates and curvatures can be added to the holder to better adapt the wedge holder to curved surfaces.

    Scan of 25.5mm HDPE plate (2530 m/s) with ACETM400 insert. PCS=82mm. Five 10mm long Vee notches

    For further information download PRODUCTS & APPLICATIONS

    Innovation Polymers

    More of Innovation Polymers published in NDT.net
    2019-04-01: Advanced Ultrasonic Couplant for Long Term Probe Placement
    2017-03-01: Low Velocity Elastomer Polymer Wedges Applied to Phased Array Probes
    2016-12-01: A Multi-Modality 3D Image Quality Assessment Standard
    2016-05-01: Low Velocity Elastomer Polymer Wedges Applied to TOFD
    2015-12-01: Acoustic Properties of the Elastomeric Materials Aqualene and ACE

  • Share...
    We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
    Accept
    top
    this is debug window