For Goodness Sake - Assuring the Quality of Toys with Thickness Gages


Olympus Scientific Solutions Americas (OSSA)216, Waltham, MA [USA]
 
NDT.net Journal
Issue: 2019-01

Inspecting plastic toys

Plastic toys are hot-ticket items during the holiday season. When shoppers are considering their purchases, safety and quality can play a role when deciding what to buy. Plastic toy manufacturers verify the quality of their products on the production line through spot checks and batch testing. The toys are also thoroughly inspected to ensure that they comply with international safety standards.

We’ve talked in the past about how XRF instruments can play a role in making toys safe, but did you know that some of our other instruments are used to help control toy quality? Toy manufacturers use instruments such as our 38DL PLUS® ultrasonic thickness gage to verify the wall thickness and uniformity of injection molded toys, which is an essential aspect of their overall quality and functionality.

Plastic Toys

Plastic is one of the most common materials used to make modern toys. Plastic is such a popular manufacturing material because it’s durable—it can usually be bent and twisted without any serious damage. Plastic is also versatile. It can be molded and used in many different ways to create a huge variety of toys. Toys made from plastic also have some advantages. They last a long time, can stand up to the rigors of play, and are easy to clean.

Pieces of an injected molded toy—some assembly required

The Thick and Thin of Injection Molding

The manufacturing process of certain toys—for example, building blocks and dress-up dolls—involves a technique called injection molding. Different types of plastic materials are injected in granular form into a precisely designed mold. The plastic is heated so it melts to a paste and lines the mold, and then it is cooled so it hardens. In the case of dolls, rotational casting, or roto-molding, is sometimes used to ensure that the plastic walls of the toys are uniform. Essentially, the mold is rotated slowly while heat is applied so the paste spreads evenly.

The raw plastic pellets used in injection molding

Manufacturing High-Quality Toys: More than Just Child’s Play

Precision for the wall thickness of these parts is critical. If the dimensions exceed the established limits, flaws and damage can occur.

Too Thick

  • The toy may not work according to the design specifications
  • It’s more expensive to manufacture (wasted raw material)
  • The toy can warp; thinner walls are actually less prone to warping

Too Thin

  • The part is less durable and won’t stand up as well to the rigors of playtime
  • It’s more expensive to produce as thinner parts require exponentially more pressure to inject the plastic paste, which wears out the mold faster

A toy’s wall thickness needs to comply with the tolerances set out in the design specs. For injection molded parts that are 1 to 20 mm thick, tolerances are as little as ±0.1 mm. Getting an accurate measurement on walls this thin was very challenging using older methods, such as cutting a sample part in half with a utility knife and measuring the thickness with a set of calipers.

How Thickness Gages Assist Quality Assurance

Toy manufacturers can use a thickness gage to perform reliable, on-the-spot quality control. The 38DL PLUS thickness gage, for example, can measure the walls of plastic parts as thin as 0.8 mm. It can provide precision measurements of the wall thickness with a standard resolution of 0.01 mm (0.001 in.) for all transducers. And it can make the measurements from just one side of the part—no cutting required.

Ultrasonic thickness gages work by measuring the time it takes for an ultrasonic sound wave to travel through the plastic part. The sound wave travels from the transducer through the part until it bounces off the opposite surface to return to the transducer. The gage measures this transit time and, using the velocity of sound in the material being measured, calculates the thickness.

To meet the demands of the production floor, the 38DL PLUS thickness gage is compact, weighing only 0.814 kg (1.80 lb), and rugged, rated IP67 dustproof and waterproof, and equipped with a protective rubber boot. Post inspection, the GageView™ interface program enables users to transfer the thickness gage’s data to spreadsheet software and other PC programs for smooth quality-control reporting.


A plastic toy injection molding factory

Summary

Given plastics’ durability, versatility of manufacturing, and relatively low cost, there’s no doubt that it will remain a popular material for making toys for many years to come. In addition to helping ensure that toys meet quality standards, thickness gages are also important for making plastic toys as green as possible. Using the minimal amount of material necessary to create a plastic toy is good for the environment, and thickness gages enable manufacturers to use minimal resources to create their products, helping ensure plastic toys remain on the shelves for many more holidays to come.

Related Content

Tags: Thickness Gage, Quality Control, Plastic

Source: InSight Blog Olympus NDT Applications Team - December 11, 2018

Olympus Scientific Solutions Americas (OSSA)

More of Olympus Scientific Solutions Americas (OSSA) published in NDT.net
2018-12-01: Train Inspection That Goes Beyond the Standard
2018-11-01: The FlexoFORM™ Scanner Provides a Complete Ultrasonic Testing Solution for Corrosion Inspection of Pipe Elbows
2018-10-01: Bridge-ing the Gap to Safety
2018-08-01: Inspection of Composite Wind Turbine Blades with Advanced Ultrasonic Phased Array Technology
2018-08-01: Inspecting Seamless Tubes with Phased Array Using the Gapless Inspection Method
2018-08-01: Adaptive Focusing Technology for the Inspection of Variable Geometry Composite Material
2018-08-01: In-service Corrosion Mapping - Challenges for the Chemical Industry
2018-08-01: Screening glass ceramic and leaded glass contaminants in glass recycling streams via handheld X-ray fluorescence (HHXRF) analyzers
2018-05-01: Olympus® and VeriPhase® Inc. Collaborate to Bring Automatic Phased Array Weld Data Processing to the NDT Market
2018-05-01: Corrosion Gage and Flaw Detector Functionality in One Instrument
All 257 Articles & News of Olympus Scientific Solutions Americas (OSSA) in NDT.net

Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window
s