Publication: 9th Conference on Industrial Computed Tomography (iCT) 2019, 13-15 Feb, Padova, Italy (iCT 2019)
Session: NDT, Materials & Manufacturing
Fri 13:50 Auditorium
ARTICLE

Combining a Computed Laminography Approach with Tomographic Analysis for a Study of Weld Joints

Marius Costin13, Caroline Vienne12, Jérôme Garnier
aLIST/DISC bDEN, DMN/SRMA; Commissariat Energie Atomique (CEA)295, Gif-Sur-Yvette, France

Abstract: The quality of a weld joint is subject to several factors, from material characteristics to environmental conditions. Its mechanical behavior is a broad field of study with specific industrial standards. Within a study of a weld joint, we employed a combination of a computed laminography [1] approach with tomographic analysis in order to extract and analyze specimens that were afterwards tested to assess the welding stress-strain and fracture characteristics. The main objective was to study the effect of surface porosity-type flaws. For this purpose, instead of a blind extraction of specimens from a welded block, we proceeded to a pre-identification of large porosity defects and the specimens were then cut and machined such that the flaws would be situated on the surface of test samples. The positions of these flaws were extracted with the laminography approach and it was crosschecked with measurements with an ultrasound testing technique. Computed tomography was employed as a characterization step before the stress-strain and fracture tests.

Keywords: weld inspection (19), X-ray CT (20), Computed laminography (7),
*Keywords are freely formed keywords from the authors and thus you may Search also for similar terms.

View:  


Feedback: ()

Share:
More from "Marius Costin" (5 of 12)
2018-08 Industrial Computed Tomography from Few Views
2018-02 Adapted acquisition trajectory and iterative reconstruction for few-views CT inspection
2017-08 L'imagerie X robotisee diversifie les strategies d'inspection
2016-07 RT Modeling for NDT Recent and Future Developments in the CIVA RT/CT Module
2016-07 X-ray Computed Tomography Reconstruction on Non-Standard Trajectories for Robotized Inspection
... All 12 Details >
More from "Caroline Vienne" (5 of 11)
2019-11 Towards a full physics radiography model
2018-08 Industrial Computed Tomography from Few Views
2018-06 Validation of CIVA RT module for nuclear applications
2018-02 Adapted acquisition trajectory and iterative reconstruction for few-views CT inspection
2017-08 L'imagerie X robotisee diversifie les strategies d'inspection
... All 11 Details >
More from "Commissariat Energie Atomique (CEA)" (5 of 294)
2020-072D Ultrasonic Antenna System for Imaging in Liquid Sodium
2020-07Design of a Phased Array EMAT for Inspection Applications in Liquid Sodium
2020-02MR sensors arrays for eddy current testing
2020-02Interpreting results of NDT/SHM methods based on elastic guided waves in composite plate-like structures by a semi-analytic modal simulation tool
2020-02Implicit-explicit scheme for the elastodynamic wave equation. Application to the modeling of guided-wave Structural Health Monitoring of anisotropic laminated plates
... All 294 Details >
Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window