"University of Stuttgart" Search Results: 4 in Date '2005-02-01'      Search  
Title / Author(s) / Keywords Session
Stress transmission in compressed granular materials evaluated by acoustic emission techniques
R. Hidalgo, F. Finck15, C. Grosse114
aInstitute for Computational Physics bInstitut für Werkstoffe im Bauwesen cInstitute of Construction Materials; University of Stuttgart285, Stuttgart , Germany
Acoutic Emission (AE)

Calibration of Sensors, Equipment
Monitoring techniques based on wireless AE sensors for large structures in civil engineering
F. Finck15, C. Grosse114, J. Kurz47, H. Reinhardt31
aInstitut für Werkstoffe im Bauwesen bInstitute of Construction Materials; University of Stuttgart285, Stuttgart , Germany
Acoutic Emission (AE)

Calibration of Sensors, Equipment
Poster
Similarity matrices as a new feature for acoustic emission analysis of concrete
F. Finck15, C. Grosse114, J. Kurz47, H. Reinhardt31
aInstitut für Werkstoffe im Bauwesen bInstitute of Construction Materials; University of Stuttgart285, Stuttgart , Germany
Acoutic Emission (AE)

Poster
Wave Propagation and Location
Investigation of fracture processes using moment tensor inversion technique
F. Finck15, C. Grosse114, H. Reinhardt31
aInstitut für Werkstoffe im Bauwesen bInstitute of Construction Materials; University of Stuttgart285, Stuttgart , Germany
Acoutic Emission (AE)

Wave Propagation and Location
   
Actual Cooperations
Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window