Evaluation of bonding quality in CFRP composite laminates by measurements of local vibration nonlinearity
I. Solodov145, D. Segur28, M. Kreutzbruck1127
1Institute for Polymer Technology (IKT); University of Stuttgart271, Stuttgart , Germany
2LIST; CEA , Toulouse, France

 