2016-04 AeroNDT 2015, Acoustic Methods for Composite Materials & Structures
A State Space Approach for the Non-Destructive Evaluation of CFRP with Ultrasonic Testing
C. Brandt15, P. Maaß22
1Airbus Operations GmbH66, Bremen, Germany
2Zentrum für Techno-mathematik; University of Bremen14, Bremen, Germany
Ultrasonic Testing (UT), aerospace, porosity, CFRP, Aircraft, stochastic, carbon fibre reinforced polymers (CFRP), periodic, back-wall echo, back-wall echo equivalent, Recurrence Plot, delay embedding, randomness, Recurrence Quantification Analysis (RQA)

 
Acoustic Methods for Composite Materials & Structures2016-04
   