where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -
NDT-Slovenia 2009

10th International Conference of the Slovenian Society for NDT, September 1-3, 2009, Ljubljana, Slovenia

Share ...     

Keywords Authors & Institutions
"National Taiwan University of Science and Technology (NTUST)" Search Results: 1 in Date '2009-10-01'      Search  
Title / Author(s) / Keywords Session
Ultrasonic Testing
A Non-Destructive Estimation on Engineering Properties of Slag Concrete Beams After Elevated Temperature
H. Wang8, S. Chen, B. Chen, T. Chang2
aDept. of Construction Engineering bDepartment of Construction Engineering; National Taiwan University of Science and Technology (NTUST)6, Taipei, Taiwan, Province of China
Ultrasonic Testing (UT), velocity, civil engineering, concrete, high temperature, moisture, strength, slag