"University of Perugia ,Terni" Search Results: 11
Filter Results ...
Publications
ECNDT 2018 (6)
AeroNDT 2018 (4)
QIRT 2018 (4)
AIPnD 2007 (3)
QIRT 2014 (3)
Art 2008 (2)
QIRT 2010 (1)
ECNDT 2014 (1)
NDT Review (1)

Languages
English (22)
Italian (3)

Title / Author(s) / Keywords PublicationDate
2019-05 QIRT 2018 Image & Data Processing
Comparison of optimization strategies for the improvement of depth detection capability of Pulse Compression Thermography
H. Malekmohammadi13, S. Laureti14, L. Senni13, P. Burrascano14, M. Ricci27
1Dept. of Engineering; University of Perugia ,Terni11, Terni, Italy
2Department of Informatics, Modeling, Electronics and System Engineering; University of Calabria (Unical)23, Calabria, Italy
Infrared Testing (IRT), pulse-compression, windowing, matched filter, 3D printed PMMA

QIRT 2018
Session: Image & Data Processing
2019-05
2019-03 AeroNDT 2018 Applications
The Use of Pulse Compression Technique in Non-Destructive Testing: A Review
M. Rizwan12, H. Malekmohammadi23, S. Laureti14, P. Burrascano24, D. Hutchins39, G. Tian429, J. ZHU44, Q. Yi44, M. Ricci27
1Dept. of Engineering; University of Perugia ,Terni11, Terni, Italy
2Dept. of Engineering; University of Perugia, Perugia, Italy
3Warwick Manufacturing Group (WMG); University of Warwick52, Coventry, United Kingdom
4University of Newcastle31, Newcastle upon Tyne, United Kingdom

AeroNDT 2018
Session: Applications
2019-03
2019-03 AeroNDT 2018 EU PhD Programme "NDT on Air" (Special Session)
Quantitative evaluation of delamination depth in CFRP based on pulse compression eddy current pulse thermography
Q. Yi14, G. Tian129, J. ZHU14, S. Laureti24, H. Malekmohammadi23, M. Ricci37
1Department of Electrical and Electronic Engineering; University of Newcastle31, Newcastle upon Tyne, United Kingdom
2Dept. of Engineering; University of Perugia ,Terni11, Terni, Italy
3DIMES; University of Calabria (Unical)23, Calabria, Italy
Pulse Compression, Eddy Current Pulsed Thermography, Quantitative evaluation, CFRP, Delamination depth

AeroNDT 2018
Session: EU PhD Programme "NDT on Air" (Special Session)
2019-03
2018-08 ECNDT 2018 Data Processing - ET
Optimizing Ultrasonic Forgings Inspection by combining Pulse-Compression technique, multi-frequency AVG analysis and phased-array probes
M. Rizwan12, L. Senni13, S. Laureti14, P. Burrascano14, M. Ricci2,37
1Dept. of Engineering; University of Perugia ,Terni11, Terni, Italy
2DIMES; University of Calabria (Unical)23, Calabria, Italy
Castings and Forgings, Iron and steel industry, Phased arrays, Steel, Ultrasonics, Defects, Power Generation

ECNDT 2018
Session: Data Processing - ET
2018-08
2018-08 ECNDT 2018 Thermography and Thermosonics Applications
Advanced methods based on active thermography for fast inspection of cast iron exhaust manifolds used in the automotive industry
F. Freni17, R. Marsili2, R. Montanini19, A. Quattrocchi13, A. Di giacomo12, G. Rossi22
1University of Messina23, Messina, Italy
2University of Perugia ,Terni11, Terni, Italy
Castings and Forgings, Infrared, Quality control, Thermography

ECNDT 2018
Session: Thermography and Thermosonics Applications
2018-08
2017-02 NDT Review Nondestructive testing and evaluation (Taylor & Francis)
Ultrasonic NDE of thick polyurethane flexible riser stiffener material
I. Mohamed12, D. Hutchins19, L. Davis13, S. Laureti12, M. Ricci27
1School of Engineering; University of Warwick52, Coventry, United Kingdom
2Dipartimento di Ingegneria; University of Perugia ,Terni11, Terni, Italy
Pulse compression, cross correlation, piezocomposite, polyurethane, SAFT

NDT Review
Session: Nondestructive testing and evaluation (Taylor & Francis)
2017-02
2015-05 QIRT 2014 Image & Data Processing
Application of pseudo - orthogonal codes at the Stimulated - Thermography Non Destructive Testing
P. Burrascano4, L. Senni3, M. Ricci7
University of Perugia ,Terni11, Terni, Italy
NDT-wide, Other Methods, Laser excited thermography, active infrared thermography, swept coded excitation, pulse compression
QIRT 2014
Session: Image & Data Processing
2015-05
2014-12 ECNDT 2014 Ultrasonic Testing (UT)
Pulse Compression Ultrasonic Non Destructive Evaluation of Thick Polymer Samples
I. Mohamed12, D. Hutchins19, L. Davis13, S. Laureti12, M. Ricci27
1School of Engineering; University of Warwick52, Coventry, United Kingdom
2University of Perugia ,Terni11, Terni, Italy
Ultrasonic Testing (UT),

ECNDT 2014
Session: Ultrasonic Testing (UT)
2014-12
2011-02 QIRT 2010 Nondestructive Evaluation & Testing
Ultrasound lockin thermography as a quantitative technique for quality control assessment of cast iron turbine components
R. Montanini19, G. Rossi22, F. Freni17
1Department of Industrial Chemistry and Materials Engineering; University of Messina23, Messina, Italy
2Department of Industrial Engineering; University of Perugia ,Terni11, Terni, Italy
Infrared Testing (IRT), thermal NDT, ultrasound thermography, casting
QIRT 2010
Session: Nondestructive Evaluation & Testing
2011-02
2009-01 AIPnD 2007 Prove di tenuta e ricerca perdite
Monitoraggio in continuo di sistemi di condotte in pressione
B. Brunone, M. Ferrante, S. Meniconi
Dipartimento di Ingegneria Civile ed Ambientale; University of Perugia ,Terni11, Terni, Italy
Leak Testing (LT), aqueducts
IT
AIPnD 2007
Session: Prove di tenuta e ricerca perdite
2009-01
2008-09 Art 2008 Imaging Methods and Monitoring: Buildings
Integrated Surveys for the Analysis of the Deterioration in the Crypt of the Abbey of Montecorona ? Italy
R. Cataldo1, S. Siviero1, G. Leucci1, R. Pagiotti2, P. Angelini2
1Department of Science of Materials; University of Salento6, Lecce, Italy
2Department of Vegetal Biology and agro-environmental and zoo technical biotechnologies; University of Perugia ,Terni11, Terni, Italy
Art 2008
Session: Imaging Methods and Monitoring: Buildings
2008-09
   
Actual Cooperations
Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window