where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -
DIR 2015 |Website| by NDT.net

Digital Industrial Radiology and Computed Tomography (DIR 2015), 22-25 June 2015, Belgium, Ghent

Share ...     

Keywords Authors & Institutions
"Brno University of Technology (BUT)" Search Results: 1 in Date '2015-08-01'      Search  
Resource Sponsors

Sponsorship inquiry contact

Title / Author(s) / Keywords Session
Poster
Application of micro-CT testing in the analysis of the silicate matrix composites
I. Kumpova115, T. Fila15, D. Vavrik119, I. Jandejsek14, Z. Kersner2
1aCentre of Excellence Telč,The Institute of Theoretical and Applied Mechanics bExcellence Telč,The Institute of Theoretical and Applied Mechanics cIEAP ; Czech Technical University (CVUT)72, Prague, Czech Republic
2Brno University of Technology (BUT)224, Brno, Czech Republic
Radiographic Testing (RT), defect detection, CT, multi-angle radiography, RTG micro-CT, dynamic defectoscopy, silicate matrix composites

Poster
   
Actual Cooperations
Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window