where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

HSNDTint 2007 |Website|

4th International Conference on NDT - October 2007 - Crete-Greece

Share ...     

Keywords Authors & Institutions
"Brno University of Technology (BUT)" Search Results: 2 in Date '2008-02-01'      Search  
Title / Author(s) / Keywords Session
HSNDTint 2007, Certification & Acoustic Emission
Determination of Uncertainty in Calibration of Acoustic Emission Sensors
J. Keprt4, P. Benesš11
Department of Control and Instrumentation; Brno University of Technology (BUT)223, Brno, Czech Republic
Acoustic Emission (AE), Primary Calibration, Sensor Calibration, Reciprocity Calibration, calibration, Measurement Uncertainty, Sensor, sensor, ASTM, Uncertainty, Czech Republic
 
Certification & Acoustic Emission
HSNDTint 2007, Poster
Application of Acoustic Emission Method for Contact Damage Identification
P. Mazal54, L. Pazder44, J. Dvoracek3
aFaculty of Mechanical Engineering bFaculty of Civil Engineering, Department of Physics; Brno University of Technology (BUT)223, Brno, Czech Republic
Acoustic Emission (AE), bearing, bearing steel, fatigue damage, Fatigue, rolling contact fatigue
 