Changes of Acoustic Emission signal and Loading Frequency during cyclic mechanical degradation of AlMg alloys
P. Mazal55
Faculty of Mechanical Engineering; Brno University of Technology (BUT)227, Brno, Czech Republic
Acoustic Emission (AE), Aluminium, Metals, fatigue damage, Fatigue Crack, fracture
   