where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -
WCNDT 2016 |Website|

19th World Conference on Non-Destructive Testing (WCNDT 2016), 13-17 June 2016 in Munich, Germany

Share ...     

Keywords Authors & Institutions
"Zetec"
Search Results: 2 in Date '2016-07-01'      Search  
Resource Sponsors


Sponsorship inquiry contact

Title / Author(s) / Keywords Session
Ultrasonic
Optimized Semi-Flexible Matrix Array Probes for Large Rotor Shafts and DGS Sizing Diagram Simulation Tool
D. Devos, G. Maes19, P. Tremblay9
Zetec86, Snoqualmie, WA, USA
Ultrasonic

Ultrasonic
Welding
Use of Sectorial Scanning for Anisotropic Weld Inspection
B. Dupont113, J. Rolland13, G. Verdeil22, J. Poirier36
1French Industrial and Mechanical Technical Centre (CETIM)92, Senlis, France
2Cameron France2, Béziers Cedex, France
3Zetec86, Snoqualmie, WA, USA