where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -
ECNDT 2014 |Website| by NDT.net

11th European Conference on Non-Destructive Testing (ECNDT 2014), Prague 2014, Oct 6-11

Share ...     

Keywords Authors & Institutions
"SIUI (Shantou Institute of Ultrasonic Instruments Co.,Ltd.)"
Search Results: 1 in Date '2014-12-01'      Search  
Resource Sponsors

Sponsorship inquiry contact

Title / Author(s) / Keywords Session
Phased Array (UT)
Application of Phased Array Ultrasonic Technique in Testing Electro-fusion Joint of Polyethylene Pipe
Y. Zheng1, W. Guo2, S. Ding24, Z. Chen1
1SIUI (Shantou Institute of Ultrasonic Instruments Co.,Ltd.)14, Shantou, China
2Zhejiang Inspection Center of Special Equipment, Hangzhou, China
Ultrasonic Testing (UT), phased array, Electro-fusion joint, polyethylene pipe