where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -
ECNDT 2018

12th European Conference on Non-Destructive Testing (ECNDT 2018), Gothenburg 2018, June 11-15

Share ...     

Keywords Authors & Institutions
"French institute of science and technology for transport, spatial planning, development and networks (IFSTTAR)" Search Results: 3 in Date '2018-08-01'      Search  
Resource Sponsors

Sponsorship inquiry contact

Title / Author(s) / Keywords Session
Civil Infrastructure-Conrete
Non Destructive Evaluation of the durability and damages of concrete in nuclear power plants.
V. Garnier127, B. Piwakowski220, J. Henault3, J. Verdier42, J. Balayssac418, N. Ranaivamonana4, J. Chaix114, S. Rakotonarivo14, G. Villian52, O. Abraham531, X. Dérobert517, C. Payan111, Z. Sbartai615, J. Saliba63, E. Larose64, H. Hafid72, R. Drelich86, C. Ciccarone8
1Laboratoire de Caractérisation Non Destructive, LCND; Aix-Marseille University (AMU)18, Marseille, France
2Ecole Centrale de Lille2, Villeneuve d'Ascq, France
3Electricité de France (EDF) R&D49, Chatou, France
4UPS, INSA; LMDC; University of Toulouse41, Toulouse, France
5French institute of science and technology for transport, spatial planning, development and networks (IFSTTAR)24, Bouguenais, France
6University Bordeaux88, Talence, France
7Mistras Group, SAS19, Sucy-en-Brie, France
8Kazimierz Wielki University9, Bydgoszcz, Poland
Civil engineering, Concrete, Defects, Monitoring, Nuclear industry, Ultrasonics

Civil Infrastructure-Conrete
Civil Infrastructure-Conrete
Imaging of a water front progression in concrete, using coda wave interferometry
R. Thery12, J. Legland15, O. Abraham131, O. Durand114, G. Villian12, E. Larose24
1aGeoEND bIFSTTAR cMast Lames; French institute of science and technology for transport, spatial planning, development and networks (IFSTTAR)24, Bouguenais, France
2ISTerre; Université Joseph Fourier de Grenoble6, Grenoble, France
Ultrasonic Testing (UT), concrete, water content, Ultrasonics, Coda Wave Interferometry

Civil Infrastructure-Conrete
Nonlinear Ultrasonics
Influence of moisture on the estimation of nonlinear parameters in concrete with Nonlinear ultrasonic Coda Wave Interferometry
J. Legland15, R. Thery12, O. Abraham131, G. Villain223, O. Durand114, E. Larose34, V. Tournat47
1aGERS bIFSTTAR; French institute of science and technology for transport, spatial planning, development and networks (IFSTTAR)24, Bouguenais, France
2IFSTTAR; Nantes Angers le Mans University (LUNAM) 39, Bouguenais, France
3ISTerre; Université Joseph Fourier de Grenoble6, Grenoble, France
4LAUM, CNRS, UMR; Université du Maine23, Le Mans, France
Concrete, Monitoring, Propagagation and scattering, Research, Ultrasonics