Nondestructive Evaluation of Historic Hakka Rammed Earth Structures
R. Liang1, G. Hota1, Y. Lei22, Y. Li2, D. Stanislawski1, Y. Jiang2
1Constructed Facilities Center; West Virginia University, Morgantown, WV, USA
2School of Architecture and Civil Engineering; Xiamen University13, Xiamen, China
Other Methods, Hakka Tulou, rammed earth, earth structures, load test, thermal comfort, NDE, nondestructive evaluation, ultrasonic, rebound hammer, Infrared thermography