where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

WCNDT 2012 |Website| by NDT.net

18th World Conference on Nondestructive Testing, April 2012, Durban, South Africa

Share ...     

Keywords Authors & Institutions
"Dresden University of Technology (TU Dresden)" Search Results: 1 in Date '2012-07-01'      Search  
Resource Sponsors

Sponsorship inquiry contact

Title / Author(s) / Keywords Session
WCNDT 2012, Materials Characterization
Evaluation of Fatigue Damage in Composite with Various Defects Using Air-coupled Guided Waves
M. Rheinfurth16, F. Schmidt22, R. Protz32, G. Busse172, P. Horst2, M. Gude34, W. Hufenbach39
1aInstitute for Polymer Testing and Polymer Science (IKP) bInstitute for Polymer Testing and Polymer Science (IKP,IKT); University of Stuttgart271, Stuttgart , Germany
2Institute of Aircraft Design and Lightweight Structures (IFL); Technische Universität Braunschweig (TU)40, Braunschweig, Germany
3aInstitut für Leichtbau und Kunststoff-technik bInstitute of Lightweight Engineering and Polymer Technology (ILK); Dresden University of Technology (TU Dresden)76, Dresden, Germany
Ultrasonic Testing (UT), Other Methods, composite, porosity, Fatigue, impact damage, Guided waves, fibre waviness, air-coupled ultrasound

 
Materials Characterization
   