2017-09 DGZfP 2017 Materialcharakterisierung
Möglichkeiten zur Extraktion akustoelastischer Konstanten aus dem Nichtlinearitätsparameter akustischer Oberflächenwellen in metallischen Werkstoffen
M. Rjelka16, B. Köhler150, A. Mayer22
1Branch Lab Dresden; Fraunhofer Institute for Ceramic Technology and System (IKTS)231, Dresden, Germany
2Hochschule Offenburg2, Offenburg, Germany