This month's issue contains articles of the 3rd International Nondestructive Testing Symposium and Exibition in

...
Turkey April 2008 and brand new articles of ULTRAGARSAS Journal of the Ultrasound Institute Kaunas (Lithuania) and of our NDT.net Journal.

During the last month we have had lively discussions about certification systems on the forum. Some of the topics raised seemed contentious and even indicated that the certification concept does not always serve its original intent of assuring a level of competence. Although we had excellent contributions for many of those "certified" we missed people of NDT societies and certifying agencies in this discussion. This forum can provide an excellent place for societies to participate and explain the systems which they offer.

New Events & Web Resources |more|
10 News in this issue
Olympus NDT Releases MXE-2.0 Software for the OmniScan Eddy Current and Eddy Current Array Flaw Detector
Olympus Scientific Solutions Americas (OSSA)
Skyray XRF Releases New Non-Destructive Analyzers to Help Increase Efficiency
Skyray XRF
World's First Handheld XRF to Include Silicon Drift Detector (SDD)
Bruker AXS GmbH
Applus RTD acquires US non-destructive testing leading group
Applus RTD
Phoenix Marks 25 Years With Move to Larger Premises
Phoenix Inspection Systems Ltd
ASNT released 'Choose NDT' Video
ASNT
Roll Alignment Diagnosis is Now Fast, Cost-Effective, and Accurate
Sensor Products Inc.
Die Diagnose der Walzenausrichtung kann nun schnell, wirtschafltich und genauestens erfolgen
Sensor Products Inc.
GE Sensing & Inspection Technologies Introduces Rhythm UT
Waygate Technologies (former GE Inspection Technologies)
Revolutionary Portable Video Borescope from GE
Waygate Technologies (former GE Inspection Technologies)
Table of Contents
27 Articles in
Issue: 2008-07-01
Title / Author(s) / Keywords Publication
open document Olympus NDT Releases MXE-2.0 Software for the OmniScan Eddy Current and Eddy Current Array Flaw Detector
Olympus Scientific Solutions Americas (OSSA)241, Waltham, MA, USA
Electromagnetic Testing (ET), eddy current testing (ECT), instrumentation, software
NEWS
NDT.net Journal
open document Skyray XRF Releases New Non-Destructive Analyzers to Help Increase Efficiency
Skyray XRF3, Georgetown, USA
Radiographic Testing (RT), x-ray fluorescence, instrumentation, materials characterization
NEWS
NDT.net Journal
open document World's First Handheld XRF to Include Silicon Drift Detector (SDD)
Bruker AXS GmbH2, Karlsruhe, Germany
Radiographic Testing (RT), x-ray fluorescence, instrumentation, materials characterization
NEWS
NDT.net Journal
open document Applus RTD acquires US non-destructive testing leading group
Applus RTD 77, Rotterdam, Netherlands
business, acquisition
NEWS
NDT.net Journal
open document Phoenix Marks 25 Years With Move to Larger Premises
Phoenix Inspection Systems Ltd71, Warrington, United Kingdom
Miscellaneous
NEWS
NDT.net Journal
open document ASNT released 'Choose NDT' Video
ASNT17, Columbus, OH, USA
NDT-wide, instrumentation, Miscellaneous, ASNT, Publication
NEWS
NDT.net Journal
open document Roll Alignment Diagnosis is Now Fast, Cost-Effective, and Accurate
Sensor Products Inc.5, Madison, USA
Other Methods, instrumentation, pressure sensing
NEWS
NDT.net Journal
open document GE Sensing & Inspection Technologies Introduces Rhythm UT
Waygate Technologies (former GE Inspection Technologies)313, Hürth, Germany
Ultrasonic Testing (UT), phased array, instrumentation, software
NEWS
NDT.net Journal
open document Revolutionary Portable Video Borescope from GE
Waygate Technologies (former GE Inspection Technologies)313, Hürth, Germany
Visual and Optical Testing (VT/OT), video borescope, instrumentation
NEWS
NDT.net Journal
3-D Data Plotting: A Useful Tool for PAUT
P. Ciorau151, L. Pullia111, W. Daks211, H. Smith27
1Inspection and Maintenance Services; Ontario Power Generation Inc.(OPG)56, Pickering, Canada
2CAD WIRE11, Markham, Ontario, Canada
Ultrasonic Testing (UT), phased array, turbine blade, weld, flaw sizing, in-situ, crack depth, defect characterization, 3-D and 2-D data plotting, rotor steeples, saturated amplitude, -6 dB cut. min-max cut, crack length

NDT.net Journal
Detection and Classification of Weld Discontinuities in Radiographic
G. Padua12, R. Da Silva27, D. Mery214, J. Rebello311, L. Calôba33
1Petrobras Research Center36, Rio de Janeiro, Brazil
2Departamento de Ciencia de la Computación; Pontificia Universidad Católica de Chile6, Santiago de Chile, Chile
3aDepartment of Electrical Engineering bDepartment of Metallurgical and Materials Engineering; Federal University of Rio de Janeiro (UFRJ)51, Rio de Janeiro, Brazil
Radiographic Testing (RT), x-ray imaging, Automated Defect Recognition ADR, Classification, imaging, weld

NDT.net Journal
Phased-Array Resolution Assessment Techniques
E. Ginzel1102, D. Johnson2
1Materials Research Institute105, Waterloo, Canada
2Eclipse Scientific Products48, Waterloo, Canada
Radiographic Testing (RT), resolution, Ultrasonic Testing (UT), phased array, beam-steering

NDT.net Journal
Ultragarsas Applications in Biology and Medicine
Ultrasonic time-of-flight method for non-invasive physiological monitoring of the human brain
A. Ragauskas1,26, G. Daubaris1,23, V. Petkus1,25, V. Deksnys1,23, J. Guzaitis1,23
1Telematics Scientific Laboratory; Ultrasound Institute at Kaunas University of Technology189, Kaunas, Lithuania
2Vittamed technologijos, Kaunas, Lithuania

Ultragarsas
Session: Applications in Biology and Medicine
Ultragarsas Nondestructive Testing and Diagnostic Methods
The review of non-destructive testing techniques suitable for inspection of the wind turbine blades
R. Raisutis35, E. Jasiuniene28, R. Sliteris26, A. Vladišauskas28
Ultrasound Institute at Kaunas University of Technology189, Kaunas, Lithuania
NDT-wide, Ultrasonic Testing (UT), wind turbine

Ultragarsas
Session: Nondestructive Testing and Diagnostic Methods
Ultragarsas Ultrasonic and Acoustic Measurements
High temperature ultrasonic transducers: review
R. Kažys58, A. Voleišis13, B. Voleišiene5
Ultrasound Institute at Kaunas University of Technology189, Kaunas, Lithuania

Ultragarsas
Session: Ultrasonic and Acoustic Measurements
Ultragarsas Ultrasonic and Acoustic Measurements
Application of ultrasonic method for investigation of porous plates
V. Jaskelevicius, G. Juodeikiene2, V. Minialga3, A. Petrauskas19
Ultrasound Institute at Kaunas University of Technology189, Kaunas, Lithuania

Ultragarsas
Session: Ultrasonic and Acoustic Measurements
Ultragarsas Ultrasonic and Acoustic Measurements
Ultrasonic flow sensor with swirl pins for flow conditioning
V. Petkus1,25, P. Borodicas1,22, A. Ragauskas1,26, V. Pamakštis1,22
1Ultrasound Institute at Kaunas University of Technology189, Kaunas, Lithuania
2Axis Industries, Kaunas, Lithuania

Ultragarsas
Session: Ultrasonic and Acoustic Measurements
Ultragarsas Wave Propagation and Vibrations
Experimental verification of the acoustic computer model using triangle reflector
E. Jasiuniene28, R. Sliteris26, L. Mažeika54
Ultrasound Institute at Kaunas University of Technology189, Kaunas, Lithuania
Ultrasonic Testing (UT), ultrasonic imaging, Simulation

Ultragarsas
Session: Wave Propagation and Vibrations
Ultragarsas Wave Propagation and Vibrations
Modelling of Lamb waves in a rectangular plate
L. Mažeika54, A. Maciulevièius2, R. Kažys58
Ultrasound Institute at Kaunas University of Technology189, Kaunas, Lithuania

Ultragarsas
Session: Wave Propagation and Vibrations
Ultragarsas Wave Propagation and Vibrations
Investigation of time-reversed ultrasonic waves focusing in multilayered media
G. Butenas3, R. Kažys58
Ultrasound Institute at Kaunas University of Technology189, Kaunas, Lithuania

Ultragarsas
Session: Wave Propagation and Vibrations
 
Page:
 -1-   2 
next pageNext
Actual Cooperations
Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window