where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -
Issue '2008-07-01'
Vol.13 No.07 - The e-Journal of Nondestructive Testing - ISSN 1435-4934
Summary

This month's issue contains articles of the 3rd International Nondestructive Testing Symposium and Exibition in

...
Turkey April 2008 and brand new articles of ULTRAGARSAS Journal of the Ultrasound Institute Kaunas (Lithuania) and of our NDT.net Journal.

During the last month we have had lively discussions about certification systems on the forum. Some of the topics raised seemed contentious and even indicated that the certification concept does not always serve its original intent of assuring a level of competence. Although we had excellent contributions for many of those "certified" we missed people of NDT societies and certifying agencies in this discussion. This forum can provide an excellent place for societies to participate and explain the systems which they offer.

New Events & Web Resources |more|
10 News in this issue
Olympus NDT Releases MXE-2.0 Software for the OmniScan Eddy Current and Eddy Current Array Flaw Detector
Olympus Scientific Solutions Americas (OSSA)
Skyray XRF Releases New Non-Destructive Analyzers to Help Increase Efficiency
Skyray XRF
World's First Handheld XRF to Include Silicon Drift Detector (SDD)
Bruker AXS GmbH
Applus RTD acquires US non-destructive testing leading group
Applus RTD
Phoenix Marks 25 Years With Move to Larger Premises
Phoenix Inspection Systems Ltd
ASNT released 'Choose NDT' Video
ASNT
Roll Alignment Diagnosis is Now Fast, Cost-Effective, and Accurate
Sensor Products Inc.
Die Diagnose der Walzenausrichtung kann nun schnell, wirtschafltich und genauestens erfolgen
Sensor Products Inc.
GE Sensing & Inspection Technologies Introduces Rhythm UT
Waygate Technologies (former GE Inspection Technologies)
Revolutionary Portable Video Borescope from GE
Waygate Technologies (former GE Inspection Technologies)
Table of Contents
21 Articles in
Issue: 2008-07-01
Filter Results ...
Exhibitors (1)
Controle Mesur.. 1
Title / Author(s) / Keywords Publication
ULUSAL VE AVRUPA STANDARDLARINDA TAHRIBATSIZ MUAYENE PERSONELI IÇIN ÖNGÖRÜLER TS 7477 EN 473, 97/23/AT EK.1-3.1.3, TS EN 10256 VE TS EN 4179, HANGISI NERDE GEREKLI
NDT Personnel in the National and International Standards
O. Pehlivanli
Turkish Standards Institution3, Kocaeli, Turkey
NDT-wide, Personnel Training and Certification, Turkey
TR
Turkey NDT 2008
KAYNAK TEKNOLOJISI VE TAHRIBATSIZ MUAYENE MERKEZI: TAHRIBATSIZ MUAYENE ÇALISMALARI
METU Welding Technology and NDT Center: NDT Activities
B. Doyum, E. Sonat, A. Doyum4, C. Gür31
aMetallurgical and Materials Engineering Dept. bDepartment of Mechanical Engineering cWelding Technology And Non-Destructive Testing Research / Application Center; Middle East Technical University (METU)42, Ankara, Turkey
Personnel Training and Certification, Turkey
TR
Turkey NDT 2008
TÜBITAK MAM?da TAHRIBATSIZ MUAYENE UYGULAMALARI ve EGITIM ETKINLIKLERI
Some NDT Applications and Training Activities at the TÜBITAK Marmara Research Center
S. Tuncel9
TÜBITAK Marmara Research Center10, Gebze / Kocaeli, Turkey
NDT-wide, accreditation laboratories, Personnel Training and Certification, Turkey
TR
Turkey NDT 2008
TURKNDT - TAHRIBATSIZ MUAYENE DERNEGI AMAÇ VE FAALIYETLER
TURKNDT - Nondestructive Testing Society: Aims and Activities
M. Yilmaz1, M. Sirin1, C. Gür2,131
1TURKNDT, Ankara, Turkey
2Metallurgical and Materials Engineering Dept.; Middle East Technical University (METU)42, Ankara, Turkey
Turkey, NDT society
TR
Turkey NDT 2008
TAHRIBATSIZ MUAYENE TEKNOLOJILERINDE SON GELISMELER: AKUSTIK EMISYON
Latest Developments in the Field of NDT Technologies: Acoustic Emission
S. Tuncel9
TÜBITAK Marmara Research Center10, Gebze / Kocaeli, Turkey
NDT-wide, Acoustic Emission (AE), Turkey
TR
Turkey NDT 2008
OTO PISTONLARININ SILINDIR GÖMLEGI KONTROL SISTEMININ TASARIMI
Designing the Automatic NDT System of Cylinder-Liner
Y. Samedov3
Bursam NDT, Bursa, Turkey
Electromagnetic Testing (ET), eddy current testing (ECT), eddy current testing probe, Automated System, automotive, steel plant, sector railway maintenance
TR
Turkey NDT 2008
ELEKTRIK DIRENÇ (YÜKSEK FREKANS) KAYNAKLI BORULARDA YÜZEY HATALARININ GIRDAP AKIMLARI (EDDY CURRENT) YÖNTEMIYLE KONTROLÜ
Detection of Surface Defects on Electrical-Resistance Welded Pipes by Eddy Currents
T. Erbay1, W. Tessa2
1Meta-Mak Metalurji Makina Mümessillik Ltd., Istanbul, Turkey
2Controle Mesure Systemes (CMS)16, La Charmee, France
Electromagnetic Testing (ET), eddy current testing (ECT), tubes and pipes, weld
TR
Turkey NDT 2008
OTOMOTIV PARÇALARININ RADYOGRAFIK INCELENMESI<br>Radiographic Investigations on Automotive Parts
A. Tugrul1, N. Baydogan1, N. Altinsoy1, D. Dizar2, E. Yagci2
1I.T.Ü. Energy Institute, Istanbul, Turkey
2Epsilon-NDT, Istanbul, Turkey
Radiographic Testing (RT), automotive
TR
Turkey NDT 2008
KAYNAK DIKISLERINDE DARBE YANKI VE TOFD TEKNIKLERININ HATA TESPIT DUYARLILIGI VE HATA BÜYÜKLÜGÜ TESPITI AÇISINDAN KARSILASTIRILMASI
Comparison of Pulse-Echo and TOFD Techniques for Probability of Detection and Estimation of Defect Size
S. Akyuz1, M. Gümrükcüoglu1, N. ÖZHAN2, H. Aras2
1TEKKON Ldt., Ankara, Turkey
2CIMTAS, Istanbul, Turkey
Ultrasonic Testing (UT), time-of-flight diffraction (TOFD), defect characterization, Probability of Detection (POD)
TR
Turkey NDT 2008
SPIRAL KAYNAKLI ÇELIK HAT BORULARININ KAYNAK DIKISLERININ RADYOSKOPIK TEST YÖNTEMI ILE MUAYENESI
Inspection of Weld Seam of Spiral Welded Pipes by Radioscopic Testing Method
Ü. AKIN, M. Nurlu2
Borusan Mannesmann Boru2, Gemlik, Turkey
Radiographic Testing (RT), tubes and pipes, weld, Spiral welded pipes
TR
Turkey NDT 2008
TARIM MAKINALARI ÜRETIMINDE ÇALISAN KAYNAKÇILARIN PROSEDÜR VE KALIFIKASYON KAYNAKLARININ TAHRIBATSIZ MUAYENESI
Application of NDT on Agricultural Machines: Qualification of Welder and Welding Procedure
S. Cengiz, S. Arin
Namik Kemal University, Tekirdag, Turkey
Agriculture, weld, welder qualification
TR
Turkey NDT 2008
YÜKSEK HIZLI HATLARDA TAHRIBATSIZ MUAYENE VE PERSONELIN VASIFLANDIRMASI DEMIRYOLU UYGULAMALARI
Nondestructive Testing Application in Railways: High Speed Railway Lines and Personnel Qualification
N. Mahmutyazicioglu4
Tahribatsýz Muayene Laboraturum; Turkish Standards Institution3, Kocaeli, Turkey
NDT-wide, railway, Personnel Training and Certification
TR
Turkey NDT 2008
HAVACILIK SEKTÖRÜNDE TAHRIBATSIZ MUAYENE UYGULAMALARINDA KALITE SISTEMININ OLUSTURULMASI
Establishing the Quality System for NDT Applications in Aviation
N. Kocer
myTECHNIC MRO, Istanbul, Turkey
NDT-wide, Electromagnetic Testing (ET), eddy current testing (ECT), Ultrasonic Testing (UT), couplant, ultrasonic couplants, aerospace, conductivity testing, corrosion testing, crack, NDT management, Qualification of Inspection, quality control
TR
Turkey NDT 2008
BOYUNA DIKISLI ÇELIK BORULARIN GIRDAP AKIMI YÖNTEMIYLE KONTROL UYGULAMALARI
Eddy Current Applications on Longitudional Welded Steel Tubes
H. Günay1, S. Karadeniz2
1TMM, Tahribatsýz Malzeme Muayene San. ve Tic. Ltd., Bursa, Turkey
2DEU, Izmir, Turkey
Electromagnetic Testing (ET), eddy current testing (ECT), eddy current, Testing, steel plant, tubes and pipes, weld, quality assurance, API, ASTM, Turkey
TR
Turkey NDT 2008
DOGALGAZ ve PETROL BORU HATLARINDA HIDROJENIN NEDEN OLDUGU ÇATLAMALAR
Hydrogen Induced Cracking in Natural Gas and Petroleum Pipelines
A. Uysal, N. Cansever
Yildiz Technical University,YTÜ4, Istanbul, Turkey
NDT-wide, Pipeline, Hydrogen induced crack (HIC)
TR
Turkey NDT 2008
DÖKÜMLERIN RADYOGRAFIK MUAYENESINDE KULLANILAN STANDARDLAR
E. Sonat, H. Yelbay7
Middle East Technical University (METU)42, Ankara, Turkey
Radiographic Testing (RT), casting, standard
TR
Turkey NDT 2008
MANYETIK BARKHAUSEN GÜRÜLTÜSÜ YÖNTEMI ILE ÇELIKLERDE TAHRIBATSIZ IÇYAPI KARAKTERIZASYONU
Nondestructive Characterization of Steel Microstructures by Magnetic Barkhausen Noise Method
C. Gür31, K. Davut4
Metallurgical and Materials Engineering Dept.; Middle East Technical University (METU)42, Ankara, Turkey
Electromagnetic Testing (ET), barkhausen noise, Steel, materials characterization, Microstructure
TR
Turkey NDT 2008
TAHRIBATSIZ YÖNTEMLERLE KALINTI GERILIM ÖLÇÜMÜNDEKI GELISMELER
Developments in Residual Stress Measurement by Nondestructive Methods
H. Yelbay7
Middle East Technical University (METU)42, Ankara, Turkey
Electromagnetic Testing (ET), barkhausen noise, Radiographic Testing (RT), neutron radiography, Ultrasonic Testing (UT), residual stress
TR
Turkey NDT 2008
KOMPOZITLERDE ORTALAMA TANECIK BOYUTUNUN ULTRASONIK ATTENUATION KATSAYISI ARASINDAKI ILISKI
Relation between Mean Grain Size and Ultrasonic Attenuation Constant in Composites
V. Özkan16, I. Sarpün15, S. Tuncel29
1Department of Physics; Afyon Kocatepe University7, Afyonkarahisar, Turkey
2TÜBITAK Marmara Research Center10, Gebze / Kocaeli, Turkey
Ultrasonic Testing (UT), attenuation, wave propagation, composite, grain size
TR
Turkey NDT 2008
SINTERLENMIS VE SINTERLENMEMIS TOZ METALURJIK PARÇALARIN ULTRASONIK YÖNTEMLE KARAKTERIZASYONU
Characterization of Green and Sintered Powder Metallurgical Parts with Ultrasonic Method
A. Topuz, H. Mollaoglu, v. Baykal
Yildiz Technical University,YTÜ4, Istanbul, Turkey
Electromagnetic Testing (ET), Ultrasonic Testing (UT), velocity, Powder metallurgy, materials characterization
TR
Turkey NDT 2008
 
Page:
 -1-   2 
next pageNext
Actual Cooperations
Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window