Issue '2010-09-01'
Vol.15 No.09 - The e-Journal of Nondestructive Testing - ISSN 1435-4934
Summary

In this month's issue we present the

...
online Workshop SimNDT 2010. The presentations in this workshop are a mix of theoretical modelling and practical simulation. In fact, not all presentations are just "technical papers". In SimNDT2010 Philippe Dubois' presentation is available as a 30 minute real-talk video. We invite you to review the presentations and to ask questions in the "Meeting Room" Special Session of the Forum. Although the whole NDT community helps to answer questions all authors of this workshop are present as well, especially to answer questions related to their presentations. As usually this issue contains more articles of individual authors.

In conjunction with this workshop a new Comment and Rating System launches for all articles and news in the database. Such a system hasn't been much applied to scientific papers up to this point. Learn more about the system in our News Release > here.

SimNDT 2010 was organized via NDTnet's freely available Event Program. For this small online Workshop the production of e-Proceedings and Abstract Booklet was not necessary, but for demonstration of this "on the fly" service, we have made both available > here. In next month's issue we will publish the e-Proceedings of the EWGAE 2010 (Sep 8-10 Vienna) which has also been successfully produced through this Event Program. As well the PANNDT 2011 Conference has started its registration process > here.

14 Articles:Online Workshop: Simulation in NDT 2010
In this month's issue we present the online Workshop SimNDT 2010. The presentations in this workshop are a mix of theoretical modelling and practical simulation. In fact, not all presentations are just "technical papers". In SimNDT2010 Philippe Dubois'
...
presentation is available as a 30 minute real-talk video. We invite you to review the presentations and to ask questions in the "Meeting Room" Special Session of the Forum. Although the whole NDT community helps to answer questions all authors of this workshop are present as well, especially to answer questions related to their presentations. Go the the Meeting Room here.
>
New Events & Web Resources |more|
8 News in this issue
NDT.net launches Comment and Rating System for Articles
NDT.net
Cokebusters Makes Clean Sweep With New Inspection Pig
Phoenix Inspection Systems Ltd
V Pan American Conference for Nondestructive Testing
5th COPAEND / PANNDT
Magnetic Analysis Corporation Expands to a New Plant
Magnetic Analysis Corp (MAC)
Newsletter August 2010
VOGT Ultrasonics GmbH
GE Automated Testing Machine Helps EUROPIPE Maintain Technology Leadership
Waygate Technologies (former GE Inspection Technologies)
GE?s ISOVOLT Titan E Helps Lufthansa Technik Create Customized Mobile X-ray Inspection Solution
Waygate Technologies (former GE Inspection Technologies)
MISTRAS Group, Inc. Awarded $3.4M Contract from the California Department of Transportation (CALTRANS)
MISTRAS Products & Systems
Table of Contents
17 Articles in
Issue: 2010-09-01
Filter Results ...
Publications
SimNDT 2010 (14)
NDT.net Journal (3)

Languages
English (15)
German (1)
Spanish (1)

Exhibitors (7)
Eclipse Scient.. 2
EXTENDE.. 1
IMASONIC SAS.. 1
Materials Rese.. 2
Zetec.. 1
Title / Author(s) / Keywords Publication
Schnelles Prüfanlagensteuerungssystem 'SPASS' in der Rohrproduktion
W. Weingarten12, G. Fischer16, S. HERRMANN2
1Salzgitter Mannesmann Forschung GmbH62, Duisburg, Germany
2Salzgitter Mannesmann Präzisrohr GmbH, Burbach-Holzhausen, Germany
Other Methods, Transport Control System, automated data collection, Automated System, Classification, visualization, detection, tubes and pipes, Process control

DE
NDT.net Journal
Fabricación de Transductores Ultrasónicos para Equipos automatizados de inspección de líneas de Tuberías
C. Rubio, O. Marrero
Centro de Ingeniería y Desarrollo Industrial (CIDESI)3, Querétaro, Mexico
Transductores de ultrasonido, PIGS, Líneas de tubería, Diablos Instrumentados, Ultrasonido

ES
NDT.net Journal
The Influence of PAUT Parameters on Crack Location, Pattern and Height Sizing
J. Poguet119, P. Ciorau251
1IMASONIC SAS31, Voray sur l'Ognon, France
2Inspection and Maintenance Services; Ontario Power Generation Inc.(OPG)56, Pickering, Canada
Fatigue Crack

NDT.net Journal
SimNDT 2010 Modeling Applications
Automated Ultrasonic Inspection of Nozzle Welds using Phased-Array Ultrasonic Testing - Part 1 - Inside Access
R. Ginzel124, E. Ginzel2102
1Eclipse Scientific Products48, Waterloo, Canada
2Materials Research Institute105, Waterloo, Canada
Ultrasonic Testing (UT), Ultrasonic Testing (UT), Ultrasonic Testing (UT), phased array, phased array, phased array, mechanised, nozzles


Appendix:
2_Ginzel.mp4 0.5 MB Movie Part 1 - Inside Access -
SimNDT 2010
Session: Modeling Applications
SimNDT 2010 Modeling Applications
Automated Ultrasonic Inspection of Nozzle Welds using Phased-Array Ultrasonic Testing - Part 2 - Outside Access
R. Ginzel124, E. Ginzel2102
1Eclipse Scientific Products48, Waterloo, Canada
2Materials Research Institute105, Waterloo, Canada
Ultrasonic Testing (UT), phased array, mechanised, nozzles

SimNDT 2010
Session: Modeling Applications
SimNDT 2010 Modeling Applications
Importance of simulations for Nuclear and Aeronautical inspections with Ultrasonic and Eddy Current Testing
E. Cuevas Aguado7, A. Garcia, F. Fernández10, J. Gadea9, J. Cordon
aNDE Innovation, Technological Development Direction bInspection Services Direction; Tecnatom S.A.94, Madrid, Spain
NDT-wide, NDT-wide, Electromagnetic Testing (ET), Electromagnetic Testing (ET), Ultrasonic Testing (UT), Ultrasonic Testing (UT), Modeling and Simulation, Modeling and Simulation, nuclear, nuclear, composite, composite, radii, aeronautical

SimNDT 2010
Session: Modeling Applications
SimNDT 2010 Modeling Applications
Microhardness Vickers and Sound Velocity in Titanium Oxide
M. Caravaca12, R. Casali22, J. Miño12
1Dpto. de Física –Química Fac. Ingeniería; Universidad Nacional del Nordeste2, Resistencia, Argentina
2Dpto. de Física, Fac. de Cs. Exactas y Naturales y Agrimensura; Universidad Nacional del Nordeste 2, Corrientes , Argentina
Modeling and Simulation, Modeling and Simulation

SimNDT 2010
Session: Modeling Applications
SimNDT 2010 Modeling Applications
Diagnostics of Fracture Processes by Measurements of Acoustic Emission
V. Khanzhin3, M. Shtremel
Metal Science and Strength Physics Department; Moscow State Institute of Steel and Alloys – MISIS (National Research Technological University)19, Moscow, Russia
acoustic emission pulse amplitude distribution, distribution approximations of acoustic emission pulse amplitude, models of distributions acoustic emission pulse amplitude, avalanche-unstable cracking, the self-organized criticality

SimNDT 2010
Session: Modeling Applications
SimNDT 2010 Modeling Applications
Brick masonry elastic modulus determination using the numerical simulation and experiments of sonic wave propagation
J. Fuente3
AIDICO3, Valencia, Spain
Ultrasonic Testing (UT), Elastic modulus, Elastic modulus, tomography, tomography, wave, wave, Rayleigh, sonic test

SimNDT 2010
Session: Modeling Applications
SimNDT 2010 Modeling Applications
Aspects of Inspection Qualification for CANDU Piping Welds
P. Ciorau51, T. Hazelton7, J. Lam6, V. Jayasinghe4, L. Pullia11, J. Coulas9
Ontario Power Generation Inc.(OPG)56, Pickering, Canada
In-Service Inspection, In-Service Inspection, ferritic piping welds, crack tilt/skew angle, inspection plan, inspection qualification, conventional UT, PAUT, weld defect pattern, length, height, ligament, CIVA simulation, ray tracing simulation, technician qualification

SimNDT 2010
Session: Modeling Applications
SimNDT 2010 Modeling Theory and Simulations
Damages in the bridges - Modeling and analysis of defects of cracks and corrosion type
S. Belattar26, N. Laaidi7
Faculty of Sciences, Laboratory of Electronics, Instrumentation and processing of the signal; Chouaib Doukkali University24, El Jadida, Morocco
Infrared Testing (IRT), infrared testing, infrared testing, Ultrasonic Testing (UT), Modelling, Modelling, Defect, Defect, Temperature, Temperature, Numeric

SimNDT 2010
Session: Modeling Theory and Simulations
SimNDT 2010 Modeling Theory and Simulations
Theory of Numerical Methods for Computer Simulation of Ultrasonic Waves Passing through the Nonlinear Flaws
V. Kniazev3
Wave Process Simulation System Laboratory Ltd.3, Moscow, Russia
Ultrasonic Testing (UT), Ultrasonic Testing (UT), Modeling and Simulation, Modeling and Simulation, Finite difference time domain (FDTD), Nonlinear waves, Nonlinear acoustic interaction, Modulation

SimNDT 2010
Session: Modeling Theory and Simulations
SimNDT 2010 Modeling Theory and Simulations
VVER RPV UT Results Modeling with ?CIVA? Software Application
I. Kadenko16, R. Iermolenko8, A. Kadenko3, N. Sakhno14
Non Destructive Examination Training and Certification Facility (NDEF)10, Kiev, Ukraine
Ultrasonic Testing (UT), Ultrasonic Testing (UT), Modeling and Simulation, Modeling and Simulation, simple slanted transducers, phased array ultrasonic transducers

SimNDT 2010
Session: Modeling Theory and Simulations
SimNDT 2010 Modeling Theory and Simulations
Capabilities and applications of the CIVA 10 modeling platform
F. Foucher27, P. Dubois10
EXTENDE101, Massy, France
Electromagnetic Testing (ET), Electromagnetic Testing (ET), Radiographic Testing (RT), Radiographic Testing (RT), Ultrasonic Testing (UT), Ultrasonic Testing (UT), Modeling and Simulation, Modeling and Simulation, computer based training, computer based training

2 /2
SimNDT 2010
Session: Modeling Theory and Simulations
SimNDT 2010 Modeling Theory and Simulations
Software Tools for the Design of Phased Array UT Inspection Techniques
D. Richard7, D. Reilly6, J. Berlanger11, G. Maes19
Zetec88, Snoqualmie, WA, USA
Ultrasonic Testing (UT), Ultrasonic Testing (UT), phased array, phased array, Modeling and Simulation, Modeling and Simulation

SimNDT 2010
Session: Modeling Theory and Simulations
SimNDT 2010 Modeling Theory and Simulations
The Essential Role of Simulation in Optimizing Probes and Inspection Strategies
G. Neau4, D. Hopkins2
BERCLI3, Berkeley, CA, USA
NDT-wide, NDT-wide, Electromagnetic Testing (ET), CIVA, CIVA, Ultrasonic Testing (UT), Ultrasonic Testing (UT), phased array, phased array, Composites, Composites, Modeling and Simulation, Modeling and Simulation, weld, weld

SimNDT 2010
Session: Modeling Theory and Simulations
SimNDT 2010 Modeling Theory and Simulations
Simulation of Time-of-Flight Diffraction (ToFD) Technique by Finite Element Method
F. Honarvar1,226, S. Khorasani1
1aFaculty of Mechanical Engineering, NDE Lab bMechanical Engineering; K. N. Toosi University of Technology (KNT)27, Tehran, Iran
2Mechanical and Industrial Engineering; University of Toronto43, Toronto, Canada
Ultrasonic Testing (UT), Ultrasonic Testing (UT), time-of-flight diffraction (TOFD), time-of-flight diffraction (TOFD), wave propagation, wave propagation, Modeling and Simulation, Modeling and Simulation, Finite Element Method, Finite Element Method

SimNDT 2010
Session: Modeling Theory and Simulations
   
Actual Cooperations
Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window