Vol.19 No.02 - The e-Journal of Nondestructive Testing - ISSN 1435-4934
Summary

In this month issue we are publishing 185 articles of the proceedings of the 14th Asia-Pacific Conference on Nondestructive testing (APCNDT 2013), which took place in Mumbai, India, November 18-22, 2013. NDT was present at this major NDT event and
...
recorded material for the published multimedia report. We are pleased to show you 10 videos of a total of three hours, containing 8 plenary talks in full length.

We started in 2014 the work on a new web design. We hope you will like the first changes of the front page and navigation menu. For comments and suggestions please contact the editor Rolf Diederichs here.

New Events & Web Resources |more|
16 News in this issue
Multimedia Review of the APCNDT 2013
NDT.net
ECNDT 2014 3rd Announcement / Abstracts extended by 31 March 2014
CZECH Society for NDT (CNDT)
eNDT : the ultimate free mobile NDT App for IOS and Android
EXTENDE
Pipeline welds: seen, measured, quantified and approved
Optical Metrology Services (OMS)
Integrity assurance – UltraSteamLine extends high temperature inspection capabilities
Plant Integrity Ltd
Glory of India Gold Medal award winner Mr. Pardikar joins TWI India
TWI Ltd (The Welding Institute)
Vince Cable India visit promotes UK business successes
TWI Ltd (The Welding Institute)
Move to new R&D village for TWI Technology Centre (Wales)
TWI Ltd (The Welding Institute)
PROMPRYLAD LLC participated in the 14th Asia Pacific Conference on Non-Destructive Testing
Promprylad” LLC
Contrôle Mesure Systèmes will exhibit at Tube Dusseldorf on booth n° 6H39
Controle Mesure Systemes (CMS)
Technology Design at the ASNT Fall Conference
Technology Design Ltd
TÜV Rheinland Acquires OpenSky Corporation, Expands IT Infrastructure, Security Services in US
TÜV Rheinland
Imaginos NDE represents Eclipse Scientific in Europe
Imaginos NDE
Canadian Institute for NDE (CINDE) and CANDU Owners Group (COG) Announce 2014 Conference
Canadian Institute for NDE (CINDE)
CIVA Newsletter January 2014
EXTENDE
The ICNDT Journal - Volume 8 Issue No. 12
International Committee for Non-Destructive Testing (ICNDT)
Table of Contents
186 Articles in
Issue: 2014-02-01
Filter Results ...
Publications
APCNDT 2013 (185)
NDT.net Journal (1)
Exhibitors (6)
GE Inspection.. 1
Intron Plus Lt.. 1
Promprylad” LL.. 1
TWI Ltd (The W.. 3
Title / Author(s) / Keywords Publication
Paint Thickness Measurements on CFRP Automobile Parts
R. Wohlleber12, J. Hinken254
1BMW AG12, Munich, Germany
2Fachbereich Elektrotechnik; University of Applied Sciences Magdeburg Stendal (FH)33, Magdeburg, Germany
NDT.net Journal
APCNDT 2013 Digital Radiography
The Use of X-ray Digital Radiography for Earthenware Inspection
G. Suparta14, A. Louk2, G. Wiguna1
1Department of Physics; Gadjah Mada University4, Yogyakarta, Indonesia
2Department of Physics; Nusa Cendana University, Kupang, Indonesia
Radiographic Testing (RT), ceramic, Digital Radiography, Non-destructive testing, structure, earthenware

APCNDT 2013
Session: Digital Radiography
APCNDT 2013 Poster
The Feasibility of Rayleigh Guided Wave Utilization for Remote Inspection of Hotspots in Bent Pipes
T. Polom1, P. Rajagopal233, M. Haq12, L. Udpa117, K. Balasubramaniam2114
1aNDE Laboratory bDepartment of Electrical and Computer Engineering; Michigan State University28, East Lansing, MI, USA
2aDepartment of Mechanical Engineering and Centre for NDE bCentre for Non Destructive Evaluation and Department of Mechanical Engineering; Indian Institute of Technology Madras (IITM)135, Chennai, India
Hot bending of pipes, microcracks, Rayleigh waves, FE simulation

APCNDT 2013
Session: Poster
APCNDT 2013 Acoustic Emission
Structural Integrity Assessment of Aluminium Liquid Propellant Tanks During Proof Pressure Testing Using Acoustic Emission Technique
B. Binu6, K. Purushothaman12, J. Philip10, S. Pillai6
Vikram Sarabhai Space Centre (VSSC)58, Thiruvananthapuram /Trivandrum, India
Acoustic Emission (AE), pressure test, realtime assessment, aluminium tank
APCNDT 2013
Session: Acoustic Emission
APCNDT 2013 Acoustic Emission
Acoustic Emission of MgCl2 Droplet SCC Testing in SUS304 Stainless Steel 
M. Shiwa2
National Institute for Materials Science (NIMS)8, Tsukuba, Japan
APCNDT 2013
Session: Acoustic Emission
APCNDT 2013 Aviation
Need and challenges of NDE for assessment of military aircraft structures
S. Kale
Center for Military Airworthiness & Certification (CEMILAC), Bangalore, India
APCNDT 2013
Session: Aviation
APCNDT 2013 Aviation
Role of Non-Destructive Evaluation in Indian Space Programme
M. Prasad
Satish Dhawan Space Centre (SDSC) SHAR7, Sriharikota, India
APCNDT 2013
Session: Aviation
APCNDT 2013 Computed Radiography
Examination Of Pipe Welds By Image Plate Based Computed Radiography System
S. Das3, M. Rana2, B. Sebastian2, D. Mukherjee7, K. Abdulla3
Bhabha Atomic Research Centre (BARC)128, Mumbai, India
APCNDT 2013
Session: Computed Radiography
APCNDT 2013 Computed Radiography
Investigations on Fading Characteristics and Ghost Image Formation in Image Plates
A. Shaikh8
Solid State Physics Division; Bhabha Atomic Research Centre (BARC)128, Mumbai, India
Radiographic Testing (RT), neutron radiography, phosphor imaging plates, signal fading, Ghost image, Fading Correction
APCNDT 2013
Session: Computed Radiography
APCNDT 2013 Computed Tomography
Development Of A Large Area X-ray Tomography System
P. Sarka4, M. Pal2, A. Sinha7
Neutron & X-ray Physics Facilities; Bhabha Atomic Research Centre (BARC)128, Mumbai, India
Radiographic Testing (RT), large area inspection, CCD, 3D X-ray Tomography, waste drum
APCNDT 2013
Session: Computed Tomography
APCNDT 2013 Computed Tomography
Tomographic Imaging of Rotating Objects
S. Shakya2, G. Bable, A. Maan2, P. Munshi13
Department of Mechanical Engineering; Indian Institute of Technology (IIT)22, Kanpur, India
NDT-wide, Radiographic Testing (RT), Other Methods
APCNDT 2013
Session: Computed Tomography
APCNDT 2013 Computed Tomography
A Fractal Study of Images obtained by IITK X-ray micro-CT
S. Shakya2, G. Agrawal, P. Munshi13
Nuclear Engineering & Technology Programme; Indian Institute of Technology (IIT)22, Kanpur, India
NDT-wide, Radiographic Testing (RT)
APCNDT 2013
Session: Computed Tomography
APCNDT 2013 Computed Tomography
Evaluation of Interlaminar Density Variations in Composite Radome using Computed Tomography (CT)
C. Muralidhar11, M. Subramanian7, V. Shankar4
Non Destructive Evaluation Division; Defence Research & Development Laboratory15, Hyderabad, India
APCNDT 2013
Session: Computed Tomography
APCNDT 2013 Computed Tomography
Integration of Computed Tomography and Coordinate Metrology in Reverse Engineering of Typical Ceramic Radome 
K. Singh, B. Prasad, P. Bhattacharjee
Defence Research & Development Laboratory15, Hyderabad, India
Radiographic Testing (RT), computed tomography
APCNDT 2013
Session: Computed Tomography
APCNDT 2013 Computed Tomography
High-Energy 3-D X-ray Tomography for Container Inspection
T. Fuchs26
Development Center X-ray technology (EZRT); Fraunhofer Institute for Integrated Circuits (IIS)186, Fürth, Germany
Radiographic Testing (RT), x-ray imaging, Computed Tomography, high energy x-ray, 3-d reconstruction
APCNDT 2013
Session: Computed Tomography
APCNDT 2013 Digital Radiography
Lag Signal in Digital X-ray Detectors and its Impact
D. Mishra2, V. Manoharan4
GE Global Research Center16, Bangalore, India
APCNDT 2013
Session: Digital Radiography
APCNDT 2013 Digital Radiography
High Energy Digital Radiography
B. Redmer61, S. Hohendorf5, U. Ewert213
BAM Federal Institute for Materials Research and Testing1323, Berlin, Germany
APCNDT 2013
Session: Digital Radiography
APCNDT 2013 Eddy Current Testing
Development of Eddy Current Test Technique for Detection of Garter Springs in 540 and 700 MWe Pressurized Heavy Water Reactors
A. Kumar5
Quality Assurance Division; Bhabha Atomic Research Centre (BARC)128, Mumbai, India
APCNDT 2013
Session: Eddy Current Testing
APCNDT 2013 Eddy Current Testing
Detection of Thickness Variation in Steel using Pulse Eddy Current Technique in Time Domain
H. Bapat7, G. Singh6, B. Singh2, R. Puri2, M. Bandyopadhyay7
Bhabha Atomic Research Centre (BARC)128, Mumbai, India
APCNDT 2013
Session: Eddy Current Testing
APCNDT 2013 Eddy Current Testing
Reduction of the Impact of Coatings Thickness Variation on Pulsed Eddy Current Signal
J. Li5, X. Wu20, Q. Zhang2, D. Deng5
aSchool of Mechanical Science and Engineering bState Engineering Research Center of Manufacturing Equipment Digitization; Huazhong University of Science and Technology28, Wuhan, China
APCNDT 2013
Session: Eddy Current Testing
 
Page:
 -1-   2   3   4   5   6   7   8   9   10 
next pageNext
Actual Cooperations
Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window