Summary

NDT.net would like to wish the NDT community a very happy New Year and much health, happiness and accomplishment in the coming year.
We are starting in the new Year 2017 with some exiting figures: more than 10,000 MyNDT members, more than 20,000
...
authors and more than 100 exhibitors have now registered in NDT.net during the last 20 Years. Thank you all for your continued interest and support.

New in this first month's issue is publishing of proceedings "NDT Days 2016" that contains 120 papers in three languages English, Russian and Bulgarian. "NDT Days" is an annual conference which is organized mainly by the Bulgarian NDT community. All non-English papers received English titles, abstracts and keywords. We appreciate the great editing work from the committee and the authors. Do not miss the next International Conference NDT Days 2017 that takes place from 13 - 16 June 2017 in Sozopol, Bulgaria.

NDT-Reliability 2017 Sep 4-8, Potsdam, Germany

7th European American Workshop on Reliability of NDE, Abstract submission is now open
New Events & Web Resources |more|
11 News in this issue
Phased array inspection (PAUT) of annular rings in the above ground storage tanks
Sonotron NDT
More speed for thermographic cameras with MCT detectors
InfraTec GmbH
Volume Graphics Releases Structural Mechanics Simulation for VGStudio MAX 3.0
Volume Graphics GmbH
Non-destructive Testing of WPC Planks using the Non-Ionising Direct Imaging NIDIT procedure
FI Test- und Messtechnik GmbH
Acoustic Control Systems Ltd. celebrated 25 year anniversary
Acoustic Control Systems Ltd.
Permanent Condition Monitoring at the Push of a Button
Fraunhofer-Institute for Non-Destructive Testing (IZFP)
A farewell to study, hello to future
Dresden International University (DIU)
Impressions from the meeting of the Arbeitskreis Dortmund of the DGZfP on December 6th, 2016
Karl Deutsch Pruef- und Messgeraetebau
KD Info 2. Ausgabe 2016
Karl Deutsch Pruef- und Messgeraetebau
ZfP-Zeitung Ausgabe 152
Deutsche Gesellschaft für Zerstörungsfreie Prüfung (DGZfP)
Non-Destructive Testing International Winter School 2017
Nanjing University of Aeronautics and Astronautics (NUAA)
Table of Contents
60 Articles in
Issue: 2017-01-01
Title / Author(s) / Keywords Publication
NDT Days 2016 NDT and Powder metallurgy
Корозионна Устойчивост на Композитно Покритие от Хром с Нанодиаманти Върху Синтеровани Железни Материали
Wear Resistance of Composite Coatings of Chromium and Nanodiamonds on Sintered Ferrous Materials
Petkov, V.1; Gidikova, N.1; Valov, R.1; Salamcı, E. 2; Bilgili, Z.2
1Institute of Metal Science, Equipment and Technologies,BAS, Sofia, Bulgaria
2Gazi University, Faculty of Engineering, Maltepe, Ankara
wear resistance, composite coatings,nanodiamonds

BG
NDT Days 2016
Session: NDT and Powder metallurgy
NDT Days 2016 Diagnostics of energetic systems
Изследване на Връзката Между Изменението на Температурата на Околната Среда и Вибрациите на Лагерите на Турбина от Турбокомпресорен Агрегат
Study of the Relationship Between Ambient Temperature and Vibration of the Turbine Bearings
Draganchev, H.; Pirovski, H.; Valchev, S.
steam turbine, vibration diagnostics, bearing vibrations

BG
NDT Days 2016
Session: Diagnostics of energetic systems
NDT Days 2016 NDT and Powder metallurgy
Фазови Превръщания при Хидротермално Третиране в Алкални Разтвори на Шлака от Пирометалургично Производство на Мед
Phase Transformations Under Hydrothermal Treatment in Alkaline Solutions Of Slag from Pyrometallurgical Production of Copper
Marinkov, N.1,2; Gurov, S.2; Kovacheva, D.1; Penkov, I.2; Rabadjieva, D.1; Aleksandrov, L.1; Stefanov, G.1
1Institute of General and Inorganic Chemistry,BAS,Sofia,Bulgaria
2.Institute of Metal Science Equipment and Technologies, BAS,Sofia,Bulgaria
copper slag, complex silicates, hydrothermal treatment

BG
NDT Days 2016
Session: NDT and Powder metallurgy
NDT Days 2016 NDT and Powder metallurgy
Охарактеризиране на Твърди Фази и Алкални Разтвори след Хидротермална Обработка на Медна Шлака
Characterization of Solid Phases and Alkaline Solution Obtained After Hydrothermal Processing of Copper Slag
Penkov, I.1; Marinkov, N.1,2; Gurov, S.2; Tswetkova, H.2; Gencheva, G.2; Kostova, J.1; Kovacheva, D.1; Stafanov, G.1; Markova-Velichkova, M.2
1Institute of Metal Science Equipment and Technologies, BAS,Sofia,Bulgaria
2Institute of General and Inorganic Chemistry,BAS, Sofia, Bulgaria
copper slag, uv-vis, icp-aes, rfa, mw

BG
NDT Days 2016
Session: NDT and Powder metallurgy
NDT Days 2016 NDT and Powder metallurgy
Трибологични Изследвания на Нови Български Жълти Павета”
Tribological Research of New Bulgarian Yellow Pavement
Kandeva, M.1; Lakov, L.2; Tsonev, P.3; Vasilev, V.3 ; Toncheva K.2
1Center for Tribology, Technical University-MTF, Sofia, Bulgaria
2Institute of Metal Science Equipment and Technologies, BAS,Sofia, Bulgaria
3„Rodna industriq Popovo” Ltd., Popovo, Bulgaria
tribology, friction

BG
NDT Days 2016
Session: NDT and Powder metallurgy
NDT Days 2016 NDT and Powder metallurgy
Сем Изследвания на Покрития върху Метали, Получени чрез Зол-Гел Технология
Sem Studies of Coatings on Metals, Produced by Sol-Gel Technology
Lakov, L.1; Yordanov S.1; Stambolova, I. 2; Jivov, B.1; Gidikova, N.1; Blaskov, V.2; Toncheva, K.1
1Institute of Metal Science Equipment and Technologies, BAS, Sofia, Bulgaria
2Institute of General and Inorganic Chemistry, BAS, Sofia, Bulgaria
sol-gel process, nano - dimension coatings, corrosion

BG
NDT Days 2016
Session: NDT and Powder metallurgy
NDT Days 2016 NDT in Civil Engineering
Приложение на Термографията за БK
Application of Thermography for NDT Control
Dimov, D.; Donchev. T.
1University of Architecture, Civil Engineering and Geodesy, Sofia, Bulgaria
2Kingston University,London, United Kingdom
thermovision method for ndt, quality control, detection of defects

BG
NDT Days 2016
Session: NDT in Civil Engineering
NDT Days 2016 NDT in Civil Engineering
Особености на Приемателното Изпитване на Жп Надлез на Км 1+545 по Жп Линия 4 Русе-Подкова
Peculiarity of Pre-Operational Tests of Ralway Ovrpass At Km 1+545 on Line 4 Russe-Podkova
Dimov, D.; Donchev. T.
pre-operational tests, static ahd dynamic tests, methods and technics of measuring

BG
NDT Days 2016
Session: NDT in Civil Engineering
NDT Days 2016 NDT in Civil Engineering
Обучението при Работодателя на Персонала по Контрол без Разрушаване
Job-Specific Training for Personnel for NDT
Skordev, A.
ndt, job-specific training, life-long learning, specific training

BG
NDT Days 2016
Session: NDT in Civil Engineering
NDT Days 2016 NDT in Civil Engineering
За Същността на Регулацията на Калибрирането на Техническите Средства при Контрола и Изпитването без Разрушаване
On the Nature of Regulations for Calibration the Equipment for Non-Destructive Testing and Inspetion
Skordev, A.
ndt, calibration in metrology, calibration in ndt, function check, verification, discontinuity, interval of calibration, accreditation, inspection body, ea 4/15, regulation, ndt personnel, test piece, certificate

BG
NDT Days 2016
Session: NDT in Civil Engineering
NDT Days 2016 NDT in Civil Engineering
Приложение на Радиационен Метод за Контрол без Разрушаване за Освидетелстване на Ракетни Двигатели
Application of X-Ray Radiography for Rocket Qualification
Genov, B.
ammunition life cycle, in-service ammunition qualification, non-destructive testing

BG
NDT Days 2016
Session: NDT in Civil Engineering
NDT Days 2016 NDT in Civil Engineering
Изисквания за Контрола без Разрушаване на Метални Конструкции в Строителството
Requirements for Non Destructive Inspection of Metal Structures in Construction
Skordev, A.
ndt, ndi construction, metal structures, welds, imperfection, requirements, risks, acceptance criteria,production, and operation, individual evaluation critical assessment

BG
NDT Days 2016
Session: NDT in Civil Engineering
NDT Days 2016 NDT in Nuclear Power Plants
Роля на Безразрушителния Контрол при Продължаване на Сроковете на Експлоатация на Блокове ВВЕР 1000 в АЕЦ Козлодуй”
Significance of Nondestructive Examination for Long Term Operation of Units WWER 1000 in Kozloduy NPP
Dimova, G.1
nuclear power plant, nde

BG
NDT Days 2016
Session: NDT in Nuclear Power Plants
Анализ на Движението на Потока в Отстойната Зона на Пещ Outokumpu
Analysis of the Movements of the Flow in the Settler of the Flash Smelting Furnace Outokumpu
Choshnova, D.
computer simulatiоn, flash smelting furnace outokumpu

BG
NDT Days 2016
Session: Poster
Индиректен Метод за Проследяване на Работата на Йонообменните Филтри при Химично Очистване на Водата в Промишлените Топло-Енергийни Централи
Indirect Method forTracking the Work of the Ion Exchange Filters in Chemical Purification of the Water in the Industrial Power Plants
Choshnova, D.
chemical ion exchange, industrial power plants

BG
NDT Days 2016
Session: Poster
Повишаване на Ефективността при Химично Очистване на Водата в Промишлените Топло-Енергийни Централи
Increasing Efficiency in Chemical Water Pollution in Industrial Thermal Power Plants
Choshnova, D.
chemical ion exchange, industrial power plants

BG
NDT Days 2016
Session: Poster
Математично Моделиране на Влиянието на Параметрите на Режима Върху Геометричните Размери на Шева при Ивиг Претопяване и Наномодифициране на Повърхностни Слоеве на Образци от Конструкционна Стомана
Mathematical Modeling of the Effect of Pulsed Current Tig Welding Parameters in Remelting and Nanomodification of Surface Layers of Structural Steel Specimens on the Geometric Dimensions of the Weld
Tashev, P.1; Koprinkova-Hristova, P.2; Petrov, Т.3; Kirilov, L.2; Lukarski,Y.1
1Institute of Metal Science Equipment and Technologies, BAS,Sofia,Bulgaria
2Institute of Information and Communication Technologies, BAS, Sofia, Bulgaria
3Technical University Sofia-Plovdiv,Bulgaria
modeling, neuron networks, pulsed current tig remelting, welding overlay, nano modification

BG
NDT Days 2016
Session: Poster
Математически Анализ, Обработване и Визуализиране на Експериментално Получени Резултати от Изпитване на Електросъпротивително Заварени Кръстови Съединения от Арматурна Стомана
Mathematical Analysis, Processing and Visualization of Experimental Results Obtained from Tests of Crucifrom Weld Joints of Reinforcing Steel
Tashev, P.1; Nachev, H.2; Tasheva, E.3
1Institute of Metal Science Equipment and Technologies, BAS, Sofia, Bulgaria
2Technical University Sofia, Bulgaria
3High Transport School ""T.Kableshkov“, Sofia, Bulgaria
resistance welding, cruciform weld joints, steel wire тел, reinforcing steel, matlab

BG
NDT Days 2016
Session: Poster
Оптимизация на Параметрите на Режима на Ивиг Претопяване при Наномодифициране на Повърхностни Слоеве на Детайли от Конструкционна Стомана
Optimization of the Parameters forPulsed Current Tig Remelting in Nano Modification of Surface Layers of Structural Steel Parts
Tashev, P.1; Kirilov, L.2; Petrov, Т.3; Koprinkova-Hristova,P.2; Lukarski, Y.1
1Institute of Metal Science Equipment and Technologies, BAS, Sofia,Bulgaria
2Institute of Information and Communication Technologies, BAS, Sofia, Bulgaria
3Technical University, Plovdiv,Bulgaria
optimization, pulsed current tig remelting, welding overlay, nano modification

BG
NDT Days 2016
Session: Poster
Разработване на Методика и Изпитване на Основните Параметри на Заваръчен Ротатор с Цифрово-Програмно Управление
Development of Methodology and Testing of Main Parameters of Welding Rotator with CNC
Petkova, G.1; Tashev, P.2
1High Transport School ""T.Kableshkov“,Sofia, Bulgaria
2Institute of Metal Science Equipment and Technologies, BAS, Sofia, Bulgaria
welding, welding works, mechanisation, automation, robotizat, cnc

BG
NDT Days 2016
Session: Poster
 
Page:
 -1-   2   3 
next pageNext
Actual Cooperations
Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window