where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -
Issue '2017-12-01'
Vol.22 No.12 - The e-Journal of Nondestructive Testing - ISSN 1435-4934
Summary

An exciting NDE 2017 Programme awaits you in Chennai from 14-16 Dec

Meet Rolf Diederichs from NDT.net at Eddyfi stand "Silver 3" in India. The NDE Proceedings will be published in NDT.net as usual.

Magnetic Analysis Corporation

USA, UT, ET, Other Methods, Manufacturer
New Events & Web Resources |more|
18 News in this issue
PAUT of the Fir-Tree Roots of the Turbine Blades without Demounting Out of the Turbine Disk
Sonotron NDT
Rapid PAUT of Bolts for the Fatigue / Corrosion Cracks
Sonotron NDT
CIVA 2017 is now released
EXTENDE
JIREH Industries Releases 3-Axis and Motorized Nozzle Scanners
Jireh Industries
VEO and PRISMA are now compatible with Ultis 3.2 for AIRBUS Group
Sonatest Ltd
YXLON Launches New Cheetah EVO and Cougar EVO at productronica
YXLON International GmbH
Fraunhofer researchers develop measuring system for ZF factory in Saarbrücken
Fraunhofer-Institute for Non-Destructive Testing (IZFP)
YXLON CT User Conference as International as Ever
YXLON International GmbH
CIVA Newsletter November 2017
EXTENDE
Librestream and Olympus Bring Remote NDT/RVI Experts into the Field Virtually
Olympus Scientific Solutions Americas (OSSA)
North Star Imaging Opening Inspection Lab on East Coast
North Star Imaging, Inc. (NSI)
YXLON International Receives Global Technology Award for Bringing a New Dimension to X-ray
YXLON International GmbH
KORMARINE Exhibition 2017, Busan Korea
Cygnus Instruments Ltd
Meeting NDT Professionals at the APCNDT in Singapore
Cygnus Instruments Ltd
Yvon Lemay appointed COO of PRAGMA
PRAGMA
Eddyfi Announces Exclusive Distribution and Collaboration Agreement with HTC / ISS for TubePro™ and More
Eddyfi Technologies
19th International Exhibition Defectoscopy / NDT St. Petersburg
Primexpo (ITE Group)
18th International Exhibition NDT Russia 2018
Primexpo (ITE Group)
Table of Contents
61 Articles in
Issue: 2017-12-01
Title / Author(s) / Keywords Publication
Reliability 2017 Applications in Industry
Determination of Defect Sizes with the help of Structural-Health-Monitoring Methods based on Guided Waves
K. Tschöke11, B. Weihnacht18, T. Gaul14, E. Schulze26, L. Schubert35, R. Neubeck7
Branch Material Diagnostics (MD); Fraunhofer Institute for Ceramic Technology and System (IKTS)231, Dresden, Germany
reliability

Reliability 2017
Session: Applications in Industry
Reliability 2017 Applications in Industry
A Reliability Study of Phased Array Ultrasonic Inspections Applied to Aluminothermic Welds in Rails
M. Carboni33, A. Gianneo10
Department of Mechanical Engineering; Politecnico di Milano84, Milano, Italy
reliability

Reliability 2017
Session: Applications in Industry
Reliability 2017 Applications in Industry
Concrete Test Specimen for NDE Reliability Demonstration
S. Kessler6
Centrum für Baustoffe und Materialprüfung (cbm); Technical University of Munich (TUM)120, Munich, Germany
reliability

Reliability 2017
Session: Applications in Industry
Reliability 2017 Applications in Industry
Considerations of Probability of Detection in Fracture-Critical Inspections of Forged Polished Car Rims
R. Mabuza3
Vaal University of Technology (VUT)14, Vanderbijlpark, South Africa
reliability

Reliability 2017
Session: Applications in Industry
Reliability 2017 Applications in Industry
Essential Parameters for the Visibility of IQIs and Small Indications in Digital Radiography
U. Ewert1213, U. Zscherpel1110, J. Vogel12, F. Zhang23, N. Long33, T. Nguyen32
18.3 Radiation Methods; BAM Federal Institute for Materials Research and Testing1327, Berlin, Germany
2Dresden International University (DIU)18, Dresden, Germany
3Vietnam Atomic Energy Institute (VINATOM)3, Hanoi , Vietnam
Image quality, Radiography, Radioscopy, Radiology, Imaging Plates, Computed Radiography, Digital Detector Arrays, MTF, CNR, basic spatial resolution

Reliability 2017
Session: Applications in Industry
Reliability 2017 General Reliability
From State of Science to State of the Art Reliability
D. Kanzler35
Applied Validation of NDT (AV-NDT)12, Berlin, Germany
reliability

Reliability 2017
Session: General Reliability
Reliability 2017 General Reliability
Research by the U.S. Nuclear Regulatory Commission on the Effects of Human Factors on Ultrasonic Examinations
A. D'Agostino1, S. Cumblidge110, S. Morrow1, N. Hughes1, C. Franklin1, T. Sanquist2
1US Nuclear Regulatory Commission, Washington, DC, USA
2Pacific Northwest National Laboratory (PNNL)26, Richland, WA, USA
reliability, human factors

Reliability 2017
Session: General Reliability
Reliability 2017 General Reliability
A Proposal to Enhance the Importance of Reliability in the Application of NDE and SHM
B. McGrath19, D. Gilbert24
1AMEC Amec Foster Wheeler2, Warrington, United Kingdom
2British Institute of Non-Destructive Testing,BINDT32, Northampton, United Kingdom
reliability, human factors

Reliability 2017
Session: General Reliability
Reliability 2017 Human Factors
Human Factors guidance to improve reliability of non-Destructive testing in the Offshore Oil and Gas Industry
M. Wall7
National NDT Centre; ESR Technology7, Abingdon, United Kingdom
reliability, human factors

Reliability 2017
Session: Human Factors
Reliability 2017 Human Factors
Human Factors Engineering in Manual Ultrasonic Testing
M. Dunlap, G. Selby11
Electric Power Research Institute (EPRI)95, Charlotte, NC, USA
reliability, human factors

Reliability 2017
Session: Human Factors
Reliability 2017 Human Factors
Effect of Feedback and Variation on Inspection Reliability
I. Virkkunen125, J. Haapalainen23, S. Papula33, T. Sarikka33, J. Kotamies3, H. Hänninen32
1Trueflaw Ltd.26, Espoo, Finland
2Department of Mechanical Engineering; VTT Technical Research Centre of Finland51, Espoo, Finland
3Metropolia University of Applied Sciences, Helsinki, Finland
reliability, human factors

Reliability 2017
Session: Human Factors
Reliability 2017 Human Factors
Using Remote NDE, including External Experts in the Inspection Process, to Enhance Reliability and address Todays NDE Challenges
N. Meyendorf136, R. Schallert24, S. Paul1, L. Bond15
1Center for Nondestructive Evaluation; Iowa State University26, Ames, Iowa, USA
2Fraunhofer IKTS, Berlin, Germany
reliability, human factors

1 /1
Reliability 2017
Session: Human Factors
Reliability 2017 Human Factors
Assessment of the Reliability of Phased Array NDT of Coarse Grain Component Based on Simulation
G. Ribay13, S. Mahaut233, G. Cattiaux328, T. Sollier334
1Commissariat Energie Atomique (CEA)295, Gif-Sur-Yvette, France
2LIST; Commissariat à l’Energie Atomique (CEA)9, Saclay, France
3DSR, SAMS; Institut de Radioprotection et de Sureté Nucléaire (IRSN)39, Fontenay aux Roses, France
reliability, human factors

Reliability 2017
Session: Human Factors
Reliability 2017 Human Factors
MAPOD case study – EDF feedback and perspectives
F. Billy13, L. Le Gratiet22, Y. Gélébart12, L. Granal1
1Electricité de France - EDF CEIDRE109, Saint-Denis, France
2Electricité de France (EDF) R&D49, Chatou, France
reliability, human factors

Reliability 2017
Session: Human Factors
POD Improvement of Defects in Fibre Reinforced Plastics by Use of Multiply Flash Thermography with Variable Pulse Parameters
G. Schober15, C. Kolb10, M. Werner3, D. Hoffmann9, S. Kremling9
SKZ - Das Kunststoff-Zentrum28, Würzburg, Germany
reliability

Reliability 2017
Session: Posters
Reliability 2017 Reliability Parameters
Real Defects as the Major Challenge of Useful POD Evaluations
D. Kanzler135, M. Pavlovic230
1Applied Validation of NDT (AV-NDT)12, Berlin, Germany
2BAM Federal Institute for Materials Research and Testing1327, Berlin, Germany
reliability

Reliability 2017
Session: Reliability Parameters
Reliability 2017 Reliability Parameters
NDE Reliability using Laboratory Induced Natural Fatigue Cracks
V. Rentala13, P. Mylavarapu24, J. Gautam14, V. Kumar36
1University of Hyderabad6, Hyderabad, India
2Defence Metallurgical Research Laboratory (DMRL)14, Hyderabad, India
3Nuclear Fuel Complex (NFC)18, Hyderabad, India
reliability

Reliability 2017
Session: Reliability Parameters
Reliability 2017 Reliability Parameters
A Multi-Parameter Probability of Detection (POD) Model for Flash Thermography
C. Maierhofer104, N. Rothbart6
BAM Federal Institute for Materials Research and Testing1327, Berlin, Germany
reliability

Reliability 2017
Session: Reliability Parameters
Reliability 2017 Reliability Parameters
Influencing parameters on image quality using photon counting detectors for laminography
D. Schumacher3, U. Ewert213, U. Zscherpel110
8.3 Radiation Methods; BAM Federal Institute for Materials Research and Testing1327, Berlin, Germany
reliability

Reliability 2017
Session: Reliability Parameters
NDT Canada 2017 Advancements in Eddy Current Inspection
Low Frequency Eddy Current for Detection of Sub-Surface Cracks in CF-188 Stub Flange
R. Underhill9
Department of Physics; Royal Military College of Canada (RMC)63, Kingston, Ontario, Canada

NDT Canada 2017
Session: Advancements in Eddy Current Inspection
 
Page:
 -1-   2   3   4 
next pageNext
Actual Cooperations
Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window