where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

Archive Authors Keywords


Publication Index



Select filters or/and search


Sort Pages
Check Filters!
New/Updated
NDT.net Journal
NDT Canada 2019
NDT Review
NDE-Nuclear-2019
DGZfP MTHz 2019
DGZfP 2019
DGZfP AE-2019
NDE-India 2018
more >
New/UpdatedNDT.net JournalNDT Canada 2019NDT ReviewNDE-Nuclear-2019DGZfP MTHz 2019DGZfP 2019DGZfP AE-2019NDE-India 2018 more >

Search Results: 5 in 0.05 sec Ordered by
Filter Results ...
Publications
NDE-India 2016 (3)
WCNDT 2000 (1)
NDE-India 2014 (1)
Title / Author(s) / Keywords PublicationDate
Ultrasonic and Acousto ultrasonic evaluation of polyimide pipes and its interface for Indian cryogenic rocket stages for space launch vehicles
S. Natraj7, V. Ravindran4, S. Somanathan7, N. Rajkumar5, S. Manna4, R. Sumangali4, B. Valsa4
Vikram Sarabhai Space Centre (VSSC)58, Thiruvananthapuram /Trivandrum, India
NDE-India 2016
2017-06
Finer ultrasonic evaluation of carbon – carbon vanes for Launch vehicle gas motors
S. Natraj7, V. Ravindran11, S. Somanathan7, N. Rajkumar5, S. Manna4, R. Sumangali4, B. Valsa4
Quality Division Propellants and Chemicals; Vikram Sarabhai Space Centre (VSSC)58, Thiruvananthapuram /Trivandrum, India

NDE-India 2016
2017-06
Ultrasonic inspection of nylon material used as solid rocket throat closure
S. Somanathan7, V. Ravindran11, S. Natraj7, N. Rajkumar5, S. Manna4, R. Sumangali4, B. Valsa4
Vikram Sarabhai Space Centre (VSSC)58, Thiruvananthapuram /Trivandrum, India

NDE-India 2016
2017-06
Non Destructive Evaluation of Porous, Very Low Density Materials and Their Bonds  of  Thermal / Acoustic Protection Systems for Space Launch Vehicles, Space Capsules and Other Ground applications
V. Ravindran11, S. Natraj7, S. Somanathan7, S. Manna4, R. Sumangali4, B. Valsa4
Vikram Sarabhai Space Centre (VSSC)58, Thiruvananthapuram /Trivandrum, India
NDE-India 2014
Session:
2015-06
2000-11 WCNDT 2000
Assessment of Steels ageing by Rayleigh wave velocity measurements
B. Acosta6, M. Beers3, L. Debarberis6, X. Gros, G. Manna, C. Pecorari
Institute for Energy; European Commission JRC36, Petten, Netherlands
Electromagnetic Testing (ET), Ultrasonic Testing (UT), laser ultrasound, non-contact, rayleigh wave, surface wave, velocity, grain size, materials characterization, STEAM

WCNDT 2000
2000-11
   
Actual Cooperations
Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window