where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

Archive Authors Keywords


Publication Index



Select filters or/and search


Sort Pages
Check Filters!
New/Updated
NDT.net Journal
NDT Review
NDE-Nuclear-2019
DGZfP MTHz 2019
DGZfP 2019
DGZfP AE-2019
NDE-India 2018
MMM-NDT 2019
more >
New/UpdatedNDT.net JournalNDT ReviewNDE-Nuclear-2019DGZfP MTHz 2019DGZfP 2019DGZfP AE-2019NDE-India 2018MMM-NDT 2019 more >

Search Results: 1 in 0.04 sec Ordered by
Title / Author(s) / Keywords PublicationDate
Statistical Case Study on Schmidt Hammer, Ultrasonic and Core Compression Strength Tests' Results Performed on Cores Obtained From Behbahan Cement Factory in Iran
M. Mahmoudipour
Geotechnical Department; SANO Consulting Engineers, Tehran, Iran
Acoustic Emission (AE), Ultrasonic, Ultrasonic Testing (UT), correlation, Other Methods, Schmidt hammer, statistical analysis, civil engineering, concrete, in-situ, Compressive strength, ASTM