where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

Archive Authors Keywords


Publication Index



Select filters or/and search


Sort Pages
Check Filters!
New/Updated
NDT.net Journal
NDE-India 2018
MMM-NDT 2019
QIRT 2018
ICWNDT 2018
Defektoskopie 2018
APWSHM 2018
Iran NDT 2018
more >
New/UpdatedNDT.net JournalNDE-India 2018MMM-NDT 2019QIRT 2018ICWNDT 2018Defektoskopie 2018APWSHM 2018Iran NDT 2018 more >

Search Results: 1 in 0.03 sec Ordered by
Title / Author(s) / Keywords PublicationDate
2016-06 Iran NDT 2016
The case study of applying Long Range Ultrasonic Test and two evaluation technique for corrosion detection of inaccessible pipe-rack in NIOC, Abouzar A&B petrochemical plant
M. Taghipour
Pars Leading Inspection Co. (PLI), Teheran, Iran
Ultrasonic Testing (UT), guided wave, Corrosion, dispersion curves, torsional wave, category response

 
Iran NDT 2016