where expertise comes together - since 1996 -

The Largest Open Access Portal of Nondestructive Testing (NDT)

Conference Proceedings, Articles, News, Exhibition, Forum, Network and more

where expertise comes together
- since 1996 -

Archive Authors Keywords


Publication Index



Select filters or/and search


Sort Pages
Check Filters!
New/Updated
NDT.net Journal
NDT Review
NDE-Nuclear-2019
DGZfP MTHz 2019
DGZfP 2019
DGZfP AE-2019
NDE-India 2018
MMM-NDT 2019
more >
New/UpdatedNDT.net JournalNDT ReviewNDE-Nuclear-2019DGZfP MTHz 2019DGZfP 2019DGZfP AE-2019NDE-India 2018MMM-NDT 2019 more >

Search Results: 1 in 0.02 sec Ordered by
Title / Author(s) / Keywords PublicationDate
2015-06 NDE-India 2014 Thermography
Infrared Thermography for On-line Monitoring of Pilgering of 18-Cr ODS Tubes
V. Varghese1, K. Kapoor23, D. Pramanik2, A. Surenthranathan1, T. Jayakumar36
1National Institute of Technology (NIT)2, Karnataka, India
2Nuclear Fuel Complex (NFC)18, Hyderabad, India
3Department of Atomic Energy; Indira Gandhi Centre for Atomic Research (IGCAR)103, Kalpakkam, India
Thermography , ODS Steel, Pilgering
NDE-India 2014
Session: Thermography
2015-06
   
Actual Cooperations
Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window