WCNDT 2008 Ultrasonic Testing
Fretting Cracking Ultrasonic Detection in Generator Teeth
X. Jian12, S. Smalley13, J. Knowles2
1Phoenix Inspection Systems Ltd67, Warrington, United Kingdom
2R&D Inspection Technologies; ALSTOM Power Service2, Baden, Switzerland
Ultrasonic Testing (UT), automated ultrasonic testing, B-scan, transducer array, Fatigue Crack, surface cracks
WCNDT 2008
Session: Ultrasonic Testing
WCNDT 2008 Ultrasonic Testing
Electromagnetic Acoustic Transducers for in and out of plane Ultrasonic Wave Detection
X. Jian12, S. Dixon216, K. Quirk16
1Phoenix Inspection Systems Ltd67, Warrington, United Kingdom
2Department of Physics; University of Warwick51, Coventry, United Kingdom
Ultrasonic Testing (UT), electromagnetic acoustic transducer (EMAT), non-contact ultrasound, automated ultrasonic testing, finite element method (FEM)
WCNDT 2008
Session: Ultrasonic Testing
   
Actual Cooperations
Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window