WCNDT 2008 Ultrasonic Testing
Automated Ultrasonic Pipe Weld Inspection
W. Deutsch65
Karl Deutsch Pruef- und Messgeraetebau123, Wuppertal, Germany
Ultrasonic Testing (UT), automated ultrasonic testing, tandem probe setup, steel plant, tubes and pipes, weld, LSAW pipes, Shell specification