WCNDT 2012 Poster, Materials
A study of MFL signals from a spectrum of defect geometries
N. Pearson1,211, M. Boat17, R. Priewald22, M. Pate1,24, J. Mason24
1Silverwing UK Ltd11, Swansea, United Kingdom
2School of Engineering; Swansea University13, Swansea, United Kingdom
Magnetic ux leakage (MFL), defect characteristics, defect normalisation, defect geometry

WCNDT 2012
Session: Poster, Materials
WCNDT 2012 Signal Processing, Imaging, Inverse problems
Practical limits of MFL in steel plate inspection
N. Pearson1,211, M. Boat17, R. Priewald22, M. Pate1,24, J. Mason24
1School of Engineering; Silverwing UK Ltd11, Swansea, United Kingdom
2School of Engineering; Swansea University13, Swansea, United Kingdom
Magnetic ux leakage (MFL), defect characteristics, defect normalisation, defect geometry

WCNDT 2012
Session: Signal Processing, Imaging, Inverse problems
   
Actual Cooperations
Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window