EWSHM 2016 Ultrasonic Testing
Lamb-Waves for Air-coupled Ultrasonic Testing with one-sided Access
W. Hillger72, D. Ilse29, L. Bühling31
Hillger Ing. Büro56, Braunschweig, Germany
Ultrasonic Testing (UT), aerospace, composite, guided waves (lamb waves), air-coupled ultrasonic technique, array technique, wave field imaging, defect detection