Approximate dV/dT values for some materials
E. Ginzel1102, R. Ginzel224
1Materials Research Institute105, Waterloo, Canada
2Ginzel Associates4, Williamsford, ON, Canada
ultrasonic, dV/dT, acoustic velocity, temperature