Phased Array Ultrasonic Inspection Of 25%Cr Super Duplex Stainless Steel On Subsea Manifold Piping Girth Welds In Lieu Of Radiography

Ezhilarasu Sengottuvelappan
GE Oil & Gas, Bangalore, India

Keywords: Ultrasonic Testing (UT) (4104), shear waves (43), Phased Array Ultrasonic Test (PAUT) (10), 25% Cr Super Duplex,
*Keywords are freely formed keywords from the authors and thus you may Search also for similar terms.

View:  


Feedback: () (3)

Share:
Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window