ARTICLE

Analysis of powder samples extracted from concrete structures of nuclear plants in Czech and Slovak Republic

Jan Zatloukal1, Petr Bezdicka23
1Experimental centre, Faculty of Civil Engineering; Czech Technical University (CVUT)73, Prague, Czech Republic
2ALMA Laboratory; Institute of Inorganic Chemistry of the ASCR3, Husinec-Rez, Czech Republic

View:  
Feedback: (1) (1)

Share:
More from "Petr Bezdicka" (1)
2008-09 Laboratory Powder X-Ray Microdiffraction ? The Use for Pigments and Secondary Salts Identification in Frescoes
More from "Czech Technical University (CVUT)" (5 of 72)
2019-12Experimental Setup for MPI Sensitivity Measurements: First Results
2019-06Verification and localization of defects on boiler waterwall tubes
2019-03Tomographic investigation of the gothic sculpture
2019-01Analysis of AE Source Location Precision For General Sensor Configurations
2019-01Contouring Geodetically Accurate Acoustic Emission Sources via Kernel Density Estimates
... All 72 Details >
More from "Institute of Inorganic Chemistry of the ASCR" (2)
2008-09Laboratory Powder X-Ray Microdiffraction ? The Use for Pigments and Secondary Salts Identification in Frescoes
2008-09Hand-Held XRF for the Preliminary Screening of Early Romanesque Frescoes in Slovakia
... All 2 Details >
Share...
We use technical and analytics cookies to ensure that we will give you the best experience of our website - More Info
Accept
top
this is debug window