Departments
Exhibition
Virtual Library
NDT by A-Z
Forum
Abstracts
Publication
Events
Archive
Exhibitors
Acoustic Emissi..
Airstar Inc.
AMDATA NDE Tech..
DELTA TEST GmbH
Eddy Current Te..
Envision Produc..
FORCE Institute
Guided Ultrason..
Hillger Ing. Bü..
Hocking NDT Ltd
IMASONIC S.A.
Innerspec Techn..
Inspection Port..
intelligeNDT Sy..
INTRON PLUS Ltd..
KARL DEUTSCH
Krautkrämer Gmb..
LECOEUR ELECTRO..
Lixi, Inc.
Lucid Software ..
Matec Instrumen..
Materials Resea..
Meß- und Prüfte..
NDT Internet Pu..
NORDINKRAFT
NUKEM Nutronik ..
NUSON Inspectio..
Panametrics, In..
Physical Acoust..
Q Net Quality M..
R/D Tech
RTD - Röntgen T..
ScanMaster Syst..
SLX, Inc.
SOFRATEST S.A.
Sonotron NDT
Sonovation B.V.
Technology Desi..
TSC Inspection ..
US Ultratek, In..
Vallen-Systeme ..
VOGT Werkstoffp..
YXLON Internati..
Zawada NDT
Exhibition
Details of All
Home
The e-Journal of Nondestructive Testing - ISSN: 1435-4934
Issue Vol. 7 No. 3 - March 2002 - Miss the last issue?
Advanced     

This Month's Introduction
DGZfP annual Conference CD-ROM
Inspection of Seamless Tubes

This month's issue focues on NDT in Germany, in particularly english articles of the DGZfP CD-ROM of the annual Conference on NDT which took place in May 2001 in Berlin.
We invite you to submit your papers on all NDT topics for future issues. NDT conference hosts are welcome to publish their proceedings on CD-ROM and add them to the NDT.net Database as we did with the WCNDT'00, A-PCNDT'01 and DGZfP'01. For further information please contact Rolf Diederichs at rd@ndt.net.

NDT
TOPIC

This Month's Articles
UT
Wall Thickness Measurement by Laser UT on Hot Tubes in a Rolling Mill
G. J. Deppe
UT
EMAT
Multi Test Block for Inspection of Seamless Tubes
A. Graff, N. Arzt, S. Nitsche, D. Sy
UT
Monitoring of ultrasound crack indications in experiments with cyclic loads
B. Köhler, F. Bergner, Uwe Ewert
UT
The Detectability of Improper Filled Ducts with Ultrasound Reflection Techniques
Otto Kroggel, Jan Scherzer, Reinhard Jansohn
MT
Reproducible Production of Magnetic Powder Crack Detecting Agents
W.A.K. Deutsch, R. Wagner, W. Weber
RT
Implementation of a method for Flaw Detection in Aluminium Castings
Ingo Weiske, Claudio Geisert, Dieter Filbert, Domingo Mery, Uwe Ewert
RT
Geometric Calibration of a X-ray Testing System
Domingo Mery, Claudio Geisert, Dieter Filbert

Selected
Publications
Online Fachbeiträge der ZfP Zeitung

You may discuss these Articles

NDTnet Forum

We Welcome New Members

News - Market - Technology
Plus News Elsewhere
News Archive '02 - '01 - '00 - '99 - '98 - '97 - '96
AIRSTAR INC. NEWS
In 2001 a team of enthusiastic engineers with many years of experience in ultrasonic NDT started a new company, Airstar Inc. Among them are Jan Strycek and Hanspeter Loertscher, who authored several articles about air-coupled ultrasound.

IntraSpect Related Model 5090 Automated Scanner Back-fit to R/D Tech Tomoscan Systems
AMDATA NDE Technology LLC announces the capability of back-fitting Model 5090 automated scanners to owners of TomoscanTM imaging systems originally supplied from R/D Tech Inc.

Integrated NDE C-Scan Imaging System
AMDATA NDE Technology LLC announces the availability of an integrated NDE C-Scan Imaging System.

New Ultrasonic Products
US Ultratek, Inc. has just released two ultrasonic testing boards.

German & United Kingdom Data Added To PatSearch FullText
MicroPatent expanded its full text coverage by adding national data from Germany and Great Britain to PatSearch FullText.

Departments
New Topics in Brief
Virtual Library
  • New Sites (30 days)
         Full-Text Search of now more than 700 Sites and 18 000 Pages (incl. PDF)
  • Forum
  • New Members (30 days)
        Now more than 900 members.
  • Exhibition
  • New Exhibitors (60 days)
         One Click Search through all Homepages of more than 5000 exhibitors' remote documents!
  • Abstracts
    Technical Literature - Training File (TEML)
    TEME is the English version of the database TEMA, a bibliographic database with German
    and international publications relating to the areas of technology and management.
    Publications
    no updates
    Events
  • 2002, OCT 31 - NOV 1, Brugge, Belgium Transducing Materials and Devices
         This conference is part of the SPIE's Photonics Fabrication Europe Symposium
  • 2003, SEP 7-10, Paris, FRANCE World Congress on Ultrasonics
         
  • NDT by A-Z
    New RT Chapter

    Upcoming Features                    Examples
  • APR 2002: Papers on Holographic NDT from Fringe 2001, Bremen, Germany.
  • 2002: selected papers of the "NDEsi"
  • 2002: We are not producing the 8th ECNDT CD-ROM
  • 2002: CD-ROM: The annual DGZfP Conference Weimar 6-8 May 2002
  • 2003: CD-ROM: Int. Symp. NDT in Civil Engineering (NDT-CE 2003) CD-ROM Berlin Sep 16-19 2003
  • Continuing developments of NDT by A-Z and Search facilities
  • Always selected papers of individual Authors (Call for Papers)
  • ©NDT.net by Rolf Diederichs.
    A private independent Publishing Company (About).
    webmaster@ndt.net